arXivDaily arXiv每日学术速递 周一至周五更新
感恩节,周五至周末无更新,大家顺遂。周一再来吧
arXiv 2603.23764cond-mat.mtrl-scicond-mat.mes-hall
收藏

具有非凡开关耐久性的质子转移铁电体

Proton-Transfer Ferroelectrics with Exceptional Switching Endurance

University of Nebraska-Lincoln(内布拉斯加大学林肯分校)

Bibek Tiwari, Yuanyuan Ni, Xiaoshan Xu

AI总结:

本研究通过低温度沉积与限制结晶工艺制备高结晶度的2-甲基苯并咪唑薄膜,展现出优异的开关耐久性,其质子转移机制与氢键链相关,且在无工程化结构下实现优于聚合物铁电材料的性能。

摘要:

可靠的有机铁电材料用于记忆应用需要在重复电开关下具有极高的耐久性。本文展示了一种高结晶度的2-甲基苯并咪唑(MBI)薄膜,通过低温度沉积后限制结晶(LDRC)工艺制备,在简单的Pt/MBI/Pt电容器几何结构中表现出极佳的疲劳抗性。通过Kolmogorov-Avrami-Ishibashi(KAI)模型分析开关动力学,揭示出具有毫秒级开关时间和准一维域生长特征的质子转移沿氢键链进行。基于这些动力学特性,我们实施了一种严格疲劳协议,旨在最大化开关应力,包括在约2Ec的双极开关条件下,以5毫秒脉冲进行连续操作约两周。剩余极化在首次10^4次循环内仅表现出轻微的唤醒(+10%)并在10^8次循环后最终恢复到初始值,测试受限于实验持续时间而非设备故障。这种鲁棒耐久性在未工程化的结构中实现,与聚合物铁电材料如P(VDF-TrFE)相比,后者通常依赖界面工程才能达到类似性能。LDRC带来的高结晶度与局部质子转移开关的结合,这种在极化反转过程中引入最小结构扰动的机制,使得这种出色的疲劳耐受性得以实现,突显了MBI作为简单、无氟的耐用有机铁电器件平台。

英文摘要:

Reliable organic ferroelectrics for memory applications require extreme endurance under repeated electrical switching. Here we demonstrate exceptional fatigue resistance in highly crystalline 2-methylbenzimidazole (MBI) films grown by low-temperature deposition followed by restrained crystallization (LDRC) in a simple Pt/MBI/Pt capacitor geometry. Switching kinetics analyzed using the Kolmogorov-Avrami-Ishibashi (KAI) model reveal characteristic millisecond switching times and quasi-one-dimensional domain growth associated with proton transfer along hydrogen-bond chains. Guided by these kinetics, we implemented a stringent fatigue protocol designed to maximize switching stress, involving bipolar switching at approximately 2Ec with 5 ms pulses, well beyond the characteristic switching time, for continuous operation over approximately 2 weeks. The remanent polarization exhibits only a minor wake-up (+10% within the first 10^4 cycles) and ultimately returns to approximately its initial value after 10^8 cycles, with testing limited by experimental duration rather than device failure. This robust endurance is achieved in an unengineered structure and contrasts with polymer ferroelectrics such as P(VDF-TrFE), where comparable performance typically relies on interfacial engineering. The combination of LDRC-enabled high crystallinity and localized proton-transfer switching, which introduces minimal structural perturbation during polarization reversal, enables this outstanding fatigue tolerance and highlights MBI as a simple, fluorine-free platform for durable organic ferroelectric devices.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑