摘要:

熔融石英玻璃是微机械、微流体和光学器件的首选材料,因为它具有极高的耐化学性、光学、电学和机械性能。氢氟酸湿法腐蚀,特别是缓冲氧化物腐蚀(BOE)仍然是制备熔石英玻璃基微器件的关键方法。众所周知,由于熔融玻璃的化学稳定性和极端侵蚀性的BOE特性,深熔融石英湿法蚀刻期间的保护掩模完整性是一个很大的挑战。在这里,我们提出了一种多级熔融石英玻璃微结构的制造路线的基础上,通过一个阶梯式掩模,只有一个灰度光刻步骤的深度湿法蚀刻。首先,我们提供了一个深入的综合分析的熔石英溶解机制在BOE溶液中,并计算了主要的氟化物馏分,如$HF^-_2$,$F^-$,$(HF)_2$组分在BOE溶液中作为pH值和$NH_4F:HF$比例的函数在室温下。然后,我们实验研究了BOE浓度($NH_4F:HF$从1:1到14:1)对熔融石英通过金属/光刻胶掩模蚀刻60分钟期间的掩模电阻、蚀刻速率和轮廓各向同性的影响。最后,我们展示了一个高品质的多级超过200微米的各向同性湿法刻蚀工艺的速率高达3微米/分钟,这可能是一个很大的兴趣,先进的熔融石英微器件与弯曲悬浮液,惯性质量,微通道,和通过晶圆孔。

英文摘要:

Fused silica glass is a material of choice for micromechanical, microfluidic, and optical devices due to its ultimate chemical resistance, optical, electrical, and mechanical performance. Wet etching in hydrofluoric solutions especially a buffered oxide etching (BOE) solution is still the key method for fabricating fused silica glass-based microdevices. It is well known that protective mask integrity during deep fused silica wet etching is a big challenge due to chemical stability of fused glass and extremely aggressive BOE properties. Here, we propose a multilevel fused silica glass microstructures fabrication route based on deep wet etching through a stepped mask with just a one grayscale photolithography step. First, we provide a deep comprehensive analysis of a fused quartz dissolution mechanism in BOE solution and calculate the main fluoride fractions like $HF^-_2$, $F^-$, $(HF)_2$ components in a BOE solution as a function of pH and $NH_4F:HF$ ratio at room temperature. Then, we experimentally investigate the influence of BOE concentration ($NH_4F:HF$ from 1:1 to 14:1) on the mask resistance, etch rate and profile isotropy during fused silica 60 minutes etching through a metal/photoresist mask. Finally, we demonstrate a high-quality multilevel over-200 um isotropic wet etching process with the rate up to 3 um/min, which could be of a great interest for advanced fused silica microdevices with flexure suspensions, inertial masses, microchannels, and through-wafer holes.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑