低温探测器用低收缩低电阻硅铝复合材料的材料性能

Material properties of a low contraction and resistivity silicon-aluminum composite for cryogenic detectors

Tatsuya Takekoshi, Kianhong Lee, Kah Wuy Chin, Shinsuke Uno, Toyo Naganuma, Shuhei Inoue, Yuka Niwa, Kazuyuki Fujita, Akira Kouchi, Shunichi Nakatsubo, Satoru Mima, Tai Oshima

摘要:

我们报告的低温性能的低收缩硅铝复合材料,即日本精细陶瓷SA 001,用作低温硅器件的封装结构。SA 001是一种硅-铝复合材料(75体积%的硅)并具有低的热膨胀系数($\sim$是铝的1/3)。测得SA 001的超导转变温度为1.18K,与纯铝的超导转变温度一致,可用作超导磁屏蔽材料。SA 001的剩余电阻率为0.065 $\mathrm{μΩm}$,这比等效的硅-铝复合材料低得多。浸入液氮中的SA 001的测量热收缩为$\frac{L_{293\mathrm{K}}-L_{77\mathrm{K}}}{L_{293\mathrm{K}}}=0.12$ %,这与从硅和铝的收缩的体积加权平均值获得的预期速率一致。SA 001的可加工性也通过制造壁厚为100 $\mathrm{μm}$的锥形喇叭天线阵列得到证实。这些特性适合于大尺寸超导探测器器件的封装应用。

英文摘要:

We report on the cryogenic properties of a low-contraction silicon-aluminum composite, namely Japan Fine Ceramics SA001, to use as a packaging structure for cryogenic silicon devices. SA001 is a silicon--aluminum composite material (75% silicon by volume) and has a low thermal expansion coefficient ($\sim$1/3 that of aluminum). The superconducting transition temperature of SA001 is measured to be 1.18 K, which is in agreement with that of pure aluminum, and is thus available as a superconducting magnetic shield material. The residual resistivity of SA001 is 0.065 $\mathrm{μΩm}$, which is considerably lower than an equivalent silicon--aluminum composite material. The measured thermal contraction of SA001 immersed in liquid nitrogen is $\frac{L_{293\mathrm{K}}-L_{77\mathrm{K}}}{L_{293\mathrm{K}}}=0.12$%, which is consistent with the expected rate obtained from the volume-weighted mean of the contractions of silicon and aluminum. The machinability of SA001 is also confirmed with a demonstrated fabrication of a conical feedhorn array, with a wall thickness of 100 $\mathrm{μm}$. These properties are suitable for packaging applications for large-format superconducting detector devices.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑