Effect of grain boundary state and grain size on the microstructure and mechanical properties of alumina obtained by SPS: A case of the amorphous layer on particle surface
M. S. Boldin, A. A. Popov, A. V. Nokhrin, A. A. Murashov, S. V. Shotin, V. N. Chuvil'deev, N. Yu. Tabachkova, K. E. Smetanina
The effect of temperature modes and heating rates (Vh) on the shrinkage kinetics of submicron and fine aluminum oxide powders has been studied. The objects of research comprised (i) submicron alfa-Al2O3 powder, (ii) submicron alfa-Al2O3 powder with an amorphous layer on particle surface, (iii) fine alfa-Al2O3 powder. The alumina ceramic specimens were produced by Spark Plasma Sintering (SPS). Equally fine powders (i) and (ii) were used to analyze the effect of an amorphous layer on sintering kinetics. Powders (i) and (iii) were used to analyze the effect of the initial particle size on shrinkage kinetics. Shrinkage curves were analyzed using the Young-Cutler and Coble models. It has been shown that sintering kinetics is determined by the intensity of grain boundary diffusion for submicron powders and by simultaneous lattice and grain boundary diffusion for fine powders. It has been determined that an amorphous layer on the surface of submicron alfa-Al2O3 powder affects grain boundary migration rate and the Coble equation parameters at SPS final stages. It has been suggested that abnormal characteristics of the alumina ceramics sintered from a submicron powder with an amorphous layer on the particle surface are associated with an increased concentration of defects at grain boundaries that were formed during crystallization of the amorphous layer.
Effect of interfacial Fe3O4 nanoparticles on the microstructure and mechanical properties of textured alumina densified by ultrafast high-temperature sintering
High heating rate effects in sintering: A phase-field study of La-doped alumina
Faculty of Mechanical Engineering, Kyoto Institute of Technology(京都工艺纤维大学机械工程学院);High-Performance Simulation Research Center, Kyoto Institute of Technology(京都工艺纤维大学高性能模拟研究中心)
Effect of ageing on the properties of the W-containing IRIS-TiAl alloy
研究了800 ℃时效对IRIS合金(Ti $_{49.9}$ Al $_{48}$ W $_2$ B $_{0.1}$)性能的影响。放电等离子烧结(SPS)致密化后的合金初始组织主要由片层团组成,片层团周围包裹着$γ$晶粒。通过力学性能试验,测定了时效处理后合金强度和抗蠕变性能的变化。显微结构的变化进行了研究,通过扫描和透射电子显微镜和X射线衍射。主要的组织演变包括片层区域的收缩和$β_0$相的析出,这伴随着钨的适度偏析和$α_2$片层宽度的减小。然而,这些演变是相对有限的,显微组织的稳定性被发现主要是由于钨的低扩散率。相反,在室温和高温下,测量这种时效处理对机械性能的适度影响。这样的实验结果解释和讨论的微观结构的演变和变形机制,在不同的温度下激活各种solicitations。