arXivDaily arXiv每日学术速递 周一至周五更新
arXiv 2202.08568cond-mat.mtrl-sci
收藏

粉末床熔融工艺参数对FeCrNi MEA微观结构和力学性能影响的原子动力学研究

Effect of powder bed fusion process parameters on microstructural and mechanical properties of FeCrNi MEA: An atomistic study

Ishat Raihan Jamil, Ali Muhit Mustaquim, Mahmudul Islam, Md Shajedul Hoque Thakur, Mohammad Nasim Hasan

摘要:

在我们的研究中,分子动力学(MD)模拟激光粉末床熔合(LPBF)等摩尔FeNiCr中熵合金(MEA)粉末进行。随着能够在微尺度上打印的较新LPBF技术的发展,需要更深入地了解工艺参数对所制造的FeNiCr MEA产品的微观结构和机械性能的潜在原子效应。根据以前的文献,LPBF工艺的参数已经系统地改变,包括层分辨率从1到6,激光功率从100 μW到220 μW,床温度从300 K到1200 K,激光扫描速度从0.5 μ s/ps到0.0625 μ s/ps。与先前的宏观实验结果一致,原子结果表明,使用较薄层的增材制造比使用较厚层的制造赋予更高的极限拉伸强度(UTS)。然而,后者需要较短的处理时间,但如果激光诱导温度不够高,则会导致小孔缺陷的形成。事实证明,提高温度有助于缓解这一问题。在制备过程中,通过将衬底温度提高到600 K或将激光功率提高到160 μW,观察到多排粉末的UTS增强。然而,超过这些临界极限,由于多个空位的出现,产品的UTS减小。我们目前的研究结果将有助于研究人员在纳米级增材制造产品的生产速度和强度之间找到良好的平衡。

英文摘要:

In our study, molecular dynamics (MD) simulations of laser powder bed fusion (LPBF) have been conducted on equimolar FeNiCr medium entropy alloy (MEA) powders. With the development of newer LPBF technologies capable of printing at the microscale, an even deeper understanding of the underlying atomistic effects of the process parameters on the microstructural and mechanical properties of the manufactured FeNiCr MEA products is required. In accordance with previous literature, the parameters of the LPBF process have been systematically varied, including layer resolution from 1 to 6, laser power from 100 μW to 220 μW, bed temperature from 300 K to 1200 K, and laser scan speed from 0.5 Å/ps to 0.0625 Å/ps. Consistent with prior macroscopic experimental findings, the atomistic results suggest that additive manufacturing using thinner layers imparts higher ultimate tensile strength (UTS) than fabricating with thicker layers. The latter, however, requires a shorter process time but induces keyhole defect formation if the laser-induced temperature is not sufficiently high enough. Increasing the temperature proves useful in mitigating this problem. Enhancement of UTS for the multi-rowed powders has been observed by raising the substrate temperature to 600 K or laser power to 160 μW during production. Beyond these critical limits, however, the UTS of the product diminishes due to the emergence of multiple vacancies. The results of our present study will help researchers to find a good balance between the production speed and strength of additive manufactured products at the nanoscale.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑