冷轧Cu30Zn黄铜微观组织变形机制与声学参数之间的相关性
Correlation between microstructural deformation mechanisms and acoustic parameters on a cold-rolled Cu30Zn brass
AI总结:
本研究通过超声测量和微观组织分析,揭示了冷轧Cu30Zn黄铜中位错增殖与晶粒细化对声速的竞争效应,以及非线性参数与孪晶层错概率在40%变形量时的峰值相关性。
摘要:
本研究评估了经受塑性变形的Cu30Zn黄铜板的声学参数与微观组织之间的关系。该板材先前在550 °C下退火30分钟,然后冷轧至10-70%范围内的压下量。采用脉冲回波法,对对应于九个不同压下量的九个试样分别进行了线性超声测量,记录了纵波沿厚度轴的飞行时间。随后,通过二次谐波产生进行了声学测量以确定非线性参数($β$)。X射线衍射分析显示,在40%厚度压下量时,变形孪晶持续增加并随后趋于饱和。在更高变形量下,微观组织显示出剪切带的产生和增殖,这与孪晶结构的减少和位错密度率的增加同时发生。纵波速度在20%变形量时下降了0.9%,此后持续增加2%。这些结果可以解释为倾向于降低线性声速的位错增殖与倾向于提高声速的平均晶粒尺寸减小之间的竞争。这些变化与通过XRD、维氏硬度和金相测量获得的值一致。非线性参数$β$在40%变形量时显示出显著的最大值,约为8倍水平。该最大值与同样在40%变形量时约为十倍水平的孪晶层错概率的类似最大值很好地相关。
英文摘要:
The relationship between acoustic parameters and the microstructure of a Cu30Zn brass plate subjected to plastic deformation was evaluated. The plate, previously annealed at 550 °C for 30 minutes, was cold rolled to reductions in the 10-70\% range. Using the pulse-echo method, linear ultrasonic measurements were performed on each of the nine specimens, corresponding to the nine different reductions, recording the wave times of flight of longitudinal wave along the thickness axis. Subsequently, acoustic measurements were performed to determine the nonlinear parameter ($β$) through the second harmonic generation. X-ray diffraction analysis revealed a steady increase and subsequent saturation of deformation twins at 40\% thickness reduction. At higher deformations, the microstructure revealed the generation and proliferation of shear bands, which coincided with a decrease in the twinning structure and an increase in dislocation density rate. Longitudinal wave velocity exhibited a 0.9\% decrease at 20\% deformation, followed by a continuous increase of 2\% beyond this point. These results can be rationalized as a competition between a proliferation of dislocations, which tends to decrease the linear sound velocity, and a decrease in average grain size, which tends to increase it. These variations are in agreement with the values obtained with XRD, Vickers hardness and metallography measurements. The nonlinear parameter $β$ shows a significant maximum, at the factor of 8 level, at 40\% deformation. This maximum correlates well with a similar maximum, at a factor of ten level and also at 40\% deformation, of the twinning fault probability.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。