On the effect of Re addition on microstructural evolution of a CoNi-based superalloy

P. Pandey, A. K. Sawant, B. Nithin, Z. Peng, S. K. Makineni, B. Gault, K. Chattopadhyay

摘要:

本文研究了稀土(Re)对一种新型低密度Co-Ni-Al-Mo-Nb基高温合金组织演变的影响。Re的加入显著影响了γ'相的形态、γ/γ'晶格失配和长期时效时γ/γ'相的组织稳定性。添加2at.% Re至Co-30 Ni-10Al-5 Mo-2Nb(均为原子%)在900°C下时效50小时的合金使γ/γ'晶格失配度降低了{ \approx } 40%(从+0.32%到+0.19%,在室温下测量),因此将γ'形态从立方形改变为圆角立方形沉淀。用原子探针层析(APT)分析了γ/γ'界面的成分分布,发现Re在γ相中的分配(K_Re=0.34),Mo在γ相中的分配(K_Mo=0.90)也发生了逆转。在γ/γ'界面上观察到了不均匀分布的界面过剩量Re(r_Re,范围为0.8 ~ 9.6atom.nm ~(-2))。在900°C(长达1000小时)下的粗化研究表明,γ'沉淀物的粗化仅通过蒸发-冷凝(EC)机制发生。这与在Co-30 Ni-10Al-5 Mo-2Nb合金以及一些Ni-Al基和高质量密度Co-Al-W基高温合金中观察到的相反,其中γ'沉淀物通过凝结/聚结机制粗化,γ'沿方向广泛排列<100>作为微观结构不稳定性的标志。γ'粗化速率指数(K_r)和γ/γ'界面能分别为1.41 × 10 ~(-27)m ~ 3/s和8.4mJ/m ~ 2,与Co-Al-W基高温合金相当,但低于Co-Al-W基高温合金。

英文摘要:

In this study, the effect of rhenium (Re) addition on microstructural evolution of a new low-density Co-Ni-Al-Mo-Nb based superalloy is presented. Addition of Re significantly influences the γ' precipitate morphology, the γ/γ' lattice misfit and the γ/γ' microstructural stability during long term aging. An addition of 2 at.% Re to a Co-30Ni-10Al-5Mo-2Nb (all in at.%) alloy, aged at 900°C for 50 hours, reduces the γ/γ' lattice misfit by {\approx} 40% (from +0.32% to +0.19%, measured at room temperature) and hence alters the γ' morphology from cuboidal to round-cornered cuboidal precipitates. The composition profiles across the γ/γ' interface by atom probe tomography (APT) reveals Re partitions to the γ phase (K_Re=0.34) and also results in the partitioning reversal of Mo to the γ phase (K_Mo=0.90) from the γ' precipitate. An inhomogeneous distribution of Gibbsian interfacial excess for the solute Re (Γ_Re, ranging from 0.8 to 9.6 atom.nm-2) has been observed at the γ/γ' interface. A coarsening study at 900°C (up to 1000 hours) suggests that the coarsening of γ' precipitates occurs solely by an evaporation--condensation (EC) mechanism. This is contrary to that observed in the Co-30Ni-10Al-5Mo-2Nb alloy as well as in some of the Ni-Al based and high mass density Co-Al-W based superalloys, where γ' precipitates coarsen by coagulation/coalescence mechanism with extensive alignment of γ' along <100> directions as a sign of microstructural instability. The γ' coarsening rate exponent (K_r) and γ/γ' interfacial energy are estimated to be 1.41 x 10-27 m3/s and 8.4 mJ/m2, which are comparable and lower than Co-Al-W based superalloys.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑