Towards controllable Si-doping in oxide molecular beam epitaxy using a solid SiO source: Application to $β$-Ga2O3

A. Ardenghi, O. Bierwagen, A. Falkenstein, G. Hoffmann, J. Lähnemann, M. Martin, P. Mazzolini

AI总结:

本文提出用固态SiO作为氧化物MBE的Si掺杂源,解决了传统Si源的氧化问题,在β-Ga2O3中实现了从4×10¹⁷到1.7×10²⁰ cm⁻³的宽范围可控掺杂,并分析了等离子体氧对源氧化的影响及除气恢复方法。

摘要:

针对氧化物分子束外延(MBE)中从Si源材料控制Si掺杂时存在的氧化相关问题,本文提出在常规蒸发源炉中使用固态SiO作为替代源材料。对来自源的不同温度($T_{SiO}$)下直接SiO通量($Φ_{SiO}$)的直线视场四极质谱分析证实,SiO分子以3.3 eV的激活能升华。在将源材料置于$10^{-5}$ mbar的O$_{2}$背景(典型氧化物MBE条件)之前和之后,均在真空中测量了随$T_{SiO}$变化的$Φ_{SiO}$。未观察到显著的$Φ_{SiO}$差异,表明在分子O$_{2}$中源氧化可忽略不计。将该源安装于氧等离子体辅助MBE中,生长了Si掺杂的$β$-Ga2O3层。评估了衬底处的$Φ_{SiO}$[从2.9×10$^{9}$ cm$^{-2}$s$^{-1}$($T_{SiO}$=700°C)到5.5×10$^{13}$ cm$^{-2}$s$^{-1}$($T_{SiO}$=1000°C)],并通过二次离子质谱测量了$β$-Ga2O3层中的Si浓度,凸显了氧化物MBE连续Si掺杂前所未有的可控性,即$N_{Si}$从4×10$^{17}$ cm$^{-3}$($T_{SiO}$=700°C)到1.7×10$^{20}$ cm$^{-3}$($T_{SiO}$=900°C)。对于同质外延$β$-Ga2O3层,展示了3×10$^{19}$ cm$^{-3}$的霍尔载流子浓度,与所提供的$Φ_{SiO}$($T_{SiO}$=800°C)一致。在750°C同质外延生长的$β$-Ga2O3(010)层与在550°C异质外延生长的$β$-Ga2O3(-201)层之间未发现SiO掺入差异。活化氧(等离子体)的存在导致源部分氧化及相关掺杂浓度下降(尤其在$T_{SiO}$<800°C时),并已用一个简单模型进行了初步解释。在1100°C对源进行除气可逆转该氧化。

英文摘要:

The oxidation-related issues in controlling Si doping from the Si source material in oxide molecular beam epitaxy (MBE) is addressed by using solid SiO as an alternative source material in a conventional effusion cell. Line-of-sight quadrupole mass spectrometry of the direct SiO-flux ($Φ_{SiO}$) from the source at different temperatures ($T_{SiO}$) confirmed SiO molecules to sublime with an activation energy of 3.3eV. The $T_{SiO}$-dependent $Φ_{SiO}$ was measured in vacuum before and after subjecting the source material to an O$_{2}$-background of $10^{-5}$ mbar (typical oxide MBE regime). The absence of a significant $Φ_{SiO}$ difference indicates negligible source oxidation in molecular O$_{2}$. Mounted in an oxygen plasma-assisted MBE, Si-doped $β$-Ga2O3 layers were grown using this source. The $Φ_{SiO}$ at the substrate was evaluated [from 2.9x10$^{9}$ cm$^{-2}$s$^{-1}$ ($T_{SiO}$=700°C) to 5.5x10$^{13}$ cm$^{-2}$s$^{-1}$ (T$_{SiO}$=1000°C)] and Si-concentration in the $β$-Ga2O3 layers measured by secondary ion mass spectrometry highlighting unprecedented control of continuous Si-doping for oxide MBE, i.e., $N_{Si}$ from 4x10$^{17}$ cm$^{-3}$ ($T_{SiO}$=700°C) up to 1.7x10$^{20}$ cm$^{-3}$ ($T_{SiO}$=900°C). For a homoepitaxial $β$-Ga2O3 layer an Hall charge carrier concentration of 3x10$^{19}$ cm$^{-3}$ in line with the provided $Φ_{SiO}$ ($T_{SiO}$=800°C) is demonstrated. No SiO-incorporation difference was found between $β$-Ga2O3(010) layers homoepitaxially grown at 750°C and $β$-Ga2O3(-201) layers heteroepitaxially grown at 550°C. The presence of activated oxygen (plasma) resulted in partial source oxidation and related decrease of doping concentration (particularly at $T_{SiO}$<800°C) which has been tentatively explained with a simple model. Degassing the source at 1100°C reverted the oxidation.