Charge modulations have been widely observed in cuprates, suggesting their centrality for understanding the high-$T_c$ superconductivity in these materials. However, the dimensionality of these modulations remains controversial, including whether their wavevector is unidirectional or bidirectional, and also whether they extend seamlessly from the surface of the material into the bulk. Material disorder presents severe challenges to understanding the charge modulations through bulk scattering techniques. We use a local technique, scanning tunneling microscopy, to image the static charge modulations on Bi$_{2-z}$Pb$_z$Sr$_{2-y}$La$_y$CuO$_{6+x}$. By comparing the phase correlation length $ξ_{\mathrm{CDW}}$ with the orientation correlation length $ξ_{\mathrm{orient}}$, we show that the charge modulations are more consistent with an underlying unidirectional wave vector. Using cluster techniques, we show that these locally 1D charge modulations are actually a bulk effect resulting from 3D criticality throughout the entire superconducting doping range.
Two types of nematicity in the phase diagram of the cuprate superconductor YBa$_2$Cu$_3$O$_y$
向列性已成为铜氧化物超导体的一个关键特征,但它与其他基本性质如超导性、电荷序和赝能隙的联系仍不清楚。在这里,我们使用测量的YBa $_2$ Cu $_3$ O $_y$的输运各向异性区分两种类型的向列性。第一个与近$p = 0.12$掺杂区的短程电荷密度波调制有关。它在能斯特系数中被检测到,而不是在电阻率中。第二种类型在较低掺杂时占优势,其中存在自旋调制但没有电荷调制。在这种情况下,在能斯特系数和电阻率检测的面内各向异性的发病-遵循跟踪赝能隙能量的温度掺杂相图中的线。我们讨论了两种可能的情况下,后者向列性。
Simultaneous emergence of superconductivity, inter-pocket scattering and nematic fluctuation in potassium-coated FeSe superconductor
超导性起源于电子配对。因此,费米面上的配对沟道和配对胶是理解超导体的两个关键问题。最近,在电子掺杂的FeSe超导体中发现了超过40 K的高温超导性,包括K $_x$ Fe $_{2-y}$ Se $_2$、Li $_{0.8}$ Fe $_{0.2}$ OHFeSe和单层FeSe薄膜。然而,它们的配对机制仍然存在争议。本文研究了包钾FeSe单晶电子结构的系统演化。通过在样品表面上原位蒸发钾来精确控制掺杂水平。我们发现当费米面的Lifshitz跃迁使两个电子袋之间的袋间散射打开时,超导性就出现了。在相同的掺杂浓度下,电子有序度显著降低,在较宽的掺杂范围内,电子有序度仍有较大的涨落。我们的研究结果表明,在电子掺杂的FeSe超导体的超导电性,袋间散射,和涨落之间的潜在的相关性。
Electronic Nematicity Revealed by Torque Magnetometry in Iron Arsenide EuFe$_2$(As$_{1-x}$P$_x$)$_2$
电子向列相是一种电子取向的有序性,它打破了铁磷属元素化物超导体的旋转对称性。然而,这一阶段的掺杂依赖性的普遍性和它的关系,其他的破缺订单(如超导)在不同的家庭的铁pnictides,仍然是悬而未决的问题。本文用转矩磁法研究了EuFe $_2$(As $_{1-x}$ P $_x$)$_2$在不引入外压的情况下的转动对称破缺。发现在最佳掺杂下,超导相在结构转变上方增殖并持续进入超导状态,之后它变得不存在或非常弱,与BaFe $_2$(As $_{1-x}$ P $_x$)$_2$中观察到的行为形成鲜明对比。这些测量结果表明,在超导圆顶下,接近最佳掺杂的假定量子跃迁。
Evolution of the nematic susceptibility in LaFe$_{1-x}$Co$_x$AsO
在一系列铁基超导体中识别出电子向列性提出了它与超导性和其他有序状态的关系的问题。本文报道了LaFe $_{1-x}$ Co $_x$ AsO单晶的弹性电阻率研究。所有的晶体在四方相都表现出类似Curie-Weiss的磁化率。提取的超导温度是单调抑制钴掺杂,并改变周围的最佳掺杂水平的符号,表明超导圆顶下可能的超导量子临界点。磁化率的幅值呈现出独特的双峰特征。这可以解释为不同的贡献的磁化率,这是放大在不同的掺杂水平的LaFe $_{1-x}$ Co $_x$ AsO的组合效应。
Nature of the Antiferromagnetic and Nematic Transitions in Sr$_{1-x}$Ba$_x$Fe$_{1.97}$Ni$_{0.03}$As$_2$
本文用磁化率和单轴压电阻率测量方法系统地研究了Sr $_{1-x}$ Ba $_x$ Fe $_{1.97}$ Ni $_{0.03}$ As $_2$的反铁磁和铁磁相变。当相变为一级相变时,磁化率和磁导率随温度变化的导数都出现明显的尖峰。相应地,我们表明,虽然磁和磁转变从一阶到二阶的变化与钡掺杂水平的增加,有一个狭窄的掺杂范围,前者成为二阶,但后者仍然是一阶,这是以前从未实现过的其他系统。此外,在此中间掺杂范围内,反铁磁和反铁磁转变温度变得不同,反铁磁磁化率的跳跃变得很小。我们的研究结果提供了关键的信息之间的相互作用的磁性和磁性转变。关于铁基超导体向列性微观模型的争论,这些观测结果与巡游费米子模型的磁情景非常吻合。
The effect of non-superconducting dopants (Mn, V, Cr and Cu) on the nematic fluctuations in iron-based superconductors
本文通过测量非超导Ba(Fe $_{1-x}$ TM $_{x}$)$_2$ As $_2$(TM = Cr,Mn,V和Cu)沿Fe-As-Fe方向的电阻率随压力的变化关系,系统地研究了非超导Ba(Fe $_{1-x}$ TM $_{x}$)$_2$ As $_2$的磁化率。所有样品的磁化率在高温下都表现出类似Curie-Weiss的行为,其中可以推导出与顺磁性中的居里常数类似的居里常数$A_n$。虽然所有这些掺杂剂都没有在BaFe $_2$ As $_2$中引入超导电性,但它们对超导涨落的影响是不同的。在Mn、Cr和V掺杂的样品中,$|A_n|$随着掺杂水平的增加而显著降低。另一方面,$|A_n|$随着Cu掺杂而显著增加,类似于超导Ni掺杂的BaFe $_2$ As $_2$。然而,$x$大于$0.04$,这可能与短程反铁磁秩序,生存到非常高的掺杂水平在低温下的磁化率被抑制。掺杂Mn、Cr和Cu到最佳掺杂的超导BaFe $_2$(As $_{0.69}$ P $_{0.31}$)$_2$中也强烈地降低了$|A_n|$。与那些明显表现出超导性的系统相比,如Ni,K或P掺杂的样品,我们的结果表明,自旋和自旋自由度之间有很强的联系。此外,Cr、Mn、V和Cu等掺杂抑制超导性的原因可能与抑制超导涨落有关。
Doping dependence of femtosecond quasi-particle relaxation dynamics in Ba(Fe,Co)_2As_2 single crystals: possible evidence for normal state nematic fluctuations
本文系统地研究了电子掺杂Ba(Fe_{1-x} Co_{x})_{2} As_{2}单晶的光激发准粒子弛豫和低能电子结构随Co掺杂量(0<= x <=0.11)的变化。$x$的光致反射率瞬态的演变没有突变。在斜方晶系自旋密度波(SDW)状态下,检测到与部分电荷间隙开口相关的瓶颈,类似于以前在不同SDW铁磷属元素化物中的结果。相对电荷间隙幅度随着x的增加而减小。在超导(SC)状态下,由于SC状态在亚0.5皮秒时间尺度上的部分(或完全)破坏,出现了额外的弛豫分量。根据SC组分的饱和行为,确定了最佳掺杂附近的光学SC态破坏能U_p/k_B= 0.3K/Fe。SC状态的随后相对缓慢的恢复指示干净的SC间隙。在正常状态下的瞬态反射率振幅的T-依赖性是一致的QP态密度中的赝能隙的存在。瞬态的极化各向异性表明,赝能隙的行为可能与一个破点对称性所产生的电子涨落持续到T~200 K在任何x。Eliashberg函数的二阶矩,从金属态在较高温度下的弛豫速率获得,表明中等的电子-声子耦合,λ <~0.3,随着掺杂的增加而降低。
Nematic Quantum Critical Fluctuations in BaFe$_{2-x}$Ni$_x$As$_2$
通过测量单轴压力下的面内电阻变化,系统地研究了电子掺杂铁基超导体BaFe $_{2-x}$ Ni $_x$ As $_2$中的电子涨落.虽然可以通过沿着(110)方向的测量来识别量子临界点,但由于类似的Curie-Weiss行为,量子和热临界涨落无法区分。在这里,我们发现,一个相当大的压力依赖于电阻率沿(100)方向存在于所有的掺杂水平,这是对一个简单的图片伊辛型的电阻率模型。沿(100)方向的信号在最佳掺杂时达到最大值,表明它与双量子临界涨落有关。我们的结果表明,条纹反铁磁序的热涨落占主导地位的欠掺杂区沿(110)方向。我们认为,要么有一个强耦合之间的量子临界波动和费米子,或更奇特的是,一个更高的对称性可能存在于周围的最佳掺杂。
Superconducting gap and nematic resonance at the quantum critical point observed by Raman scattering in $\mathrm{BaFe_{2}}(\mathrm{As}_{1-x}\mathrm{P}_{x}\mathrm{)_{2}}$
Simultaneous Vanishing of the Nematic Electronic State and the Structural Orthorhombicity in NaFe$_{1-x}$Co$_x$As Single Crystals
我们在单轴压力下对NaFe $_{1-x}$ Co $_x$ As单晶进行了面内电阻率测量。在掺杂水平高达约x=0.025 $\pm$ <0.002的母态和欠掺杂态中发现了平面内电阻率$ρ_a$和$ρ_b$随沿$b$ -轴的单轴压力的明显区别。从$ρ_a$和$ρ_b$的偏离点,以及电阻率的独特扭结结构,结合已发表的实验数据,确定了晶体结构转变和反铁磁转变的温度。结果清楚地表明,电子态的消失与结构的转变同时进行。然而,在较低的掺杂水平下,反铁磁状态消失。结合BaFe $_{2-x}$ Co $_x$ As $_2$的实验数据,我们的结果表明向列性与超导电性有密切的关系.
Nematic Fluctuations in the Cuprate Superconductor Bi$_2$Sr$_2$CaCu$_2$O$_{8+δ}$
在它们的相图中建立量子临界点的存在和性质是高温超导铜氧化物的核心谜团。它可以解释它们的赝能隙和奇怪的金属相,以及最终它们的高超导温度。然而,尽管在几种非常规超导体中存在与量子临界点相关的无处不在的临界涨落的确凿证据,但在铜氧化物中,它们至今仍未被发现。在这里,我们使用铜酸盐Bi $_2$ Sr $_2$ CaCu $_2$ O $_{8+δ}$中的电子拉曼散射,报告观察到增强的电子拉曼涨落附近的赝能隙相的端点。虽然我们的数据暗示可能存在一个初始的量子临界点,掺杂的依赖性的量子波动偏离一个典型的量子临界情况显着。观察到的不稳定性,而似乎是绑定到一个范霍夫奇点的存在下的能带结构。
Visualizing the interplay of dual electronic nematicities in kagome superconductors
University of Science and Technology of China(中国科学技术大学);Beijing National Laboratory for Condensed Matter Physics and Institute of Physics, Chinese Academy of Sciences(中国科学院物理研究所北京凝聚态物理国家研究中心);CAS Key Laboratory of Theoretical Physics, Institute of Theoretical Physics, Chinese Academy of Sciences(中国科学院理论物理研究所理论物理国家重点实验室);Hefei National Research Center for Physical Sciences at the Microscale, University of Science and Technology of China(中国科学技术大学微尺度物质科学国家研究中心);Hefei National Laboratory, University of Science and Technology of China(中国科学技术大学合肥国家实验室)
轨道有序最近成为铁基超导体中的另一个重要状态,它对超导性的作用以及它与磁有序和斜方晶格畸变的联系引起了激烈的争论。为了寻找这种所谓的氧磷族化合物中的超导相的特征,我们重新审视了磷族化合物超导体LaFeAsO $_{1-x}$ F $_x$的正常态性质,重点是电阻率,能斯特效应,热膨胀和$^{75}$ As NMR数据。在欠掺杂水平$x=0.05$的输运性质在与未掺杂LaFeAsO形成长程有序的温度相同的温度下,即在约160 K下,表现出明显的异常。此外,$^{75}$ As-NMR自旋-晶格弛豫速率$1/(T_1T)$揭示了自旋波动的逐渐减慢。然而,长程磁序和可检测的正交晶格畸变是不存在的。因此,我们从数据中得出结论,短程轨道有序或它的缓慢波动形式在160 K附近开始。值得注意的是,在运输中的所有异常和缓慢的自旋波动的迹象消失接近最佳掺杂$x=0.1$,这表明在LaFeAsO $_{1-x}$ F $_x$的超导相实际上竞争。
Boost of critical current density near quantum critical points in FeSe-Based superconductors with two superconducting domes
Southeast University(东南大学);Center for High Pressure Science and Technology Advanced Research (HPSTAR)(高压科学与技术先进研究中心);Jining University(济宁学院);Changshu Institute of Technology(常熟理工学院);The University of Tokyo(东京大学);Qufu Normal University(曲阜师范大学)
Structural distortion behind the nematic superconductivity in Sr$_x$Bi$_2$Se$_3$
典型的层状拓扑绝缘体Bi $_2$ Se $_3$在掺杂Sr、Nb或Cu时变成半导体。这些材料在面内磁场存在下的超导性质证明了自发对称性破缺:180 $^\circ$ -超导性的旋转对称性与120 $^\circ$ -晶体的旋转对称性。这种行为极好地证实了拓扑超导电性。这种向列性在多大程度上是由于这些材料中的超导配对,而不是由于晶体结构扭曲?这个问题仍然没有答案,因为到目前为止,在这些材料中没有明显的偏离三重晶体对称性。为了解决这个问题,我们生长高品质的单晶体的Sr $_x$ Bi $_2$ Se $_3$,进行详细的X射线衍射和磁输运研究,并揭示所观察到的超导向列性方向与这些样品中的小的结构扭曲的方向($\sim 0.02$ \%伸长率在一个结晶方向)。另外的各向异性来自微晶轴的取向。2-在远高于临界温度的最均匀的晶体中观察到的磁阻的折叠对称性表明这些结构畸变仍然足够强。我们的数据结合强样品到样品的变化的超导各向异性参数的指示的意义的结构因素在表观超导性锶$_x$ Bi $_2$ Se $_3$。
Disorder-induced damping of spin excitations in Cr-doped BaFe$_2$As$_2$
European Synchrotron Radiation Facility(欧洲同步辐射装置);Instituto de Física, Universidade de São Paulo(圣保罗大学物理研究所);Institut Quantique and Département de Physique, Université de Sherbrooke(舍布鲁克大学量子研究所与物理系);Fakultät für Chemie und Mineralogie, Universität Leipzig(莱比锡大学化学与矿物学院);School of Chemistry and Chemical Engineering, University of Surrey(萨里大学化学与化学工程学院);Diamond Light Source(钻石光源);Instituto de Física “Gleb Wataghin”, UNICAMP(坎皮纳斯大学格莱布·瓦塔金物理研究所);Département de Physique and Fribourg Center for Nanomaterials, Université de Fribourg(弗里堡大学物理系与弗里堡纳米材料中心);Photon Science Division, Paul Scherrer Institut(保罗谢尔研究所光子科学部)