用Zr K边(1 s)X射线吸收近边结构(XANES)和扩展X射线吸收精细结构(EXAFS)谱研究了ZrB_2外延薄膜中的化学键,并与合成薄膜的ZrB_2化合物靶和体相α-Zr参比进行了比较。X射线光电子能谱学的定量分析表明,在溅射清洗完成后,在ZrB 2外延膜中约有5%的O,在ZrB 2复合靶中约有19%的O,在体相α-Zr参比物中约有22%的O。对于ZrB 2化合物靶,X射线衍射(XRD)显示来自单斜晶系ZrO 2的弱但可见的~ 111、111和220峰以及来自ZrB 2的峰,并且其中ZrB 2峰的强度分布显示随机取向的靶材料。对于体相α-Zr参比,在0001取向金属记录的衍射图中未观察到任何结晶氧化物的峰。从两个ZrB 2样品的Zr的K-边吸收表现出更明显的振荡的外延ZrB 2膜比在体ZrB 2归因于高的原子有序内的列的膜。由于ZrB 2中缺乏p-d杂化,XANES没有表现出前峰,但是与从Zr到B的电荷转移的α-Zr(17.993 keV)相比,在膜中具有向更高能量的4 eV和在体中具有6 eV的化学位移。大块ZrB 2材料中的2 eV较大的位移表明比外延膜中的氧含量更高,这是由XPS支持的。在EXAFS中,与块状靶材(a = 3.175 μ m,c= 3.540 μ m)相比,薄膜中ZrB 2的模拟胞边缘(a = 3.165 μ m,c = 3.520 μ m)略小,而在六方密排金属(α相,a=3.254 μ m,c=5.147 μ m)中。

英文摘要:

The chemical bonding in an epitaxial ZrB2 film is investigated by Zr K-edge (1s) X-ray absorption near-edge structure (XANES) and extended X-ray absorption fine structure (EXAFS) spectroscopies and compared to the ZrB2 compound target from which the film was synthesized as well as a bulk α-Zr reference. Quantitative analysis of X-ray Photoelectron Spectroscopy spectra reveals at the surface: ~5% O in the epitaxial ZrB2 film, ~19% O in the ZrB2 compound target and ~22% O in the bulk α-Zr reference after completed sputter cleaning. For the ZrB2 compound target, X-ray diffraction (XRD) shows weak but visible -111, 111, and 220 peaks from monoclinic ZrO2 together with peaks from ZrB2 and where the intensity distribution for the ZrB2 peaks show a randomly oriented target material. For the bulk α-Zr reference no peaks from any crystalline oxide were visible in the diffractogram recorded from the 0001-oriented metal. The Zr K-edge absorption from the two ZrB2 samples demonstrate more pronounced oscillations for the epitaxial ZrB2 film than in the bulk ZrB2 attributed to the high atomic ordering within the columns of the film. The XANES exhibits no pre-peak due to lack of p-d hybridization in ZrB2, but with a chemical shift towards higher energy of 4 eV in the film and 6 eV for the bulk compared to α-Zr (17.993 keV) from the charge-transfer from Zr to B. The 2 eV larger shift in bulk ZrB2 material suggests higher oxygen content than in the epitaxial film, which is supported by XPS. In EXAFS, the modelled cell-edge in ZrB2 is slightly smaller in the thin film (a=3.165 Å, c=3.520 Å) in comparison to the bulk target material (a=3.175 Å, c=3.540 Å) while in hexagonal closest-packed metal (α-phase, a=3.254 Å, c=5.147 Å).

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑