锂离子电池阴极界面的纳米级电压增强

Nanoscale Voltage Enhancement at Cathode Interfaces in Li-ion Batteries

Shenzhen Xu, Ryan Jacobs, Chris Wolverton, Thomas Kuech, Dane Morgan

摘要:

界面在Li离子电池电极中普遍存在,跨越组成梯度、多相共生区域以及在电极和固体电解质界面或保护涂层之间出现。然而,这些界面对Li能量的影响在很大程度上仍然未知。在这项工作中,我们计算了锂嵌入现场能量跨阴极界面,并证明了这些能量的界面两侧的物理支配。我们研究了橄榄石/橄榄石结构的LixFePO 4/LixMPO 4(x=0和1,M=Co,Ti,Mn)和层状/层状结构的LiNiO 2/TiO 2界面,以探索不同的材料结构和过渡金属元素。我们发现,在从高电压到低电压材料的界面上,Li电压在高电压材料中保持恒定,并且在低电压区域中近似线性地衰减,接近低电压材料的Li电压。这种效应的范围为0.5- 9 nm,取决于界面偶极屏蔽。这种效应为界面处的高压材料提供了一种机制,以在纳米尺度上显著增强低压材料中的Li嵌入电压。我们发现,这种电压增强是由电子转移(从低到高电压区域),应变和界面偶极屏蔽的组合。我们探讨了这种电压增强的影响,一种新的异质结构阴极设计和氧化还原赝电容器。

英文摘要:

Interfaces are ubiquitous in Li-ion battery electrodes, occurring across compositional gradients, regions of multiphase intergrowths, and between electrodes and solid electrolyte interphases or protective coatings. However, the impact of these interfaces on Li energetics remains largely unknown. In this work, we calculated Li intercalation-site energetics across cathode interfaces and demonstrated the physics governing these energetics on both sides of the interface. We studied the olivine/olivine-structured LixFePO4/LixMPO4 (x=0 and 1, M=Co, Ti, Mn) and layered/layered-structured LiNiO2/TiO2 interfaces to explore different material structures and transition metal elements. We found that across an interface from a high- to low-voltage material the Li voltage remains constant in the high-voltage material and decays approximately linearly in the low-voltage region, approaching the Li voltage of the low-voltage material. This effect ranges from 0.5-9nm depending on the interfacial dipole screening. This effect provides a mechanism for a high-voltage material at an interface to significantly enhance the Li intercalation voltage in a low-voltage material over nanometer scale. We showed that this voltage enhancement is governed by a combination of electron transfer (from low- to high-voltage regions), strain and interfacial dipole screening. We explored the implications of this voltage enhancement for a novel heterostructured-cathode design and redox pseudocapacitors.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑