polymer玻璃中的裂纹和零应力下的演化:突出离散长时间尺度弛豫

Cracking in polymer glasses and evolution at zero stress: Highlighting discrete long time scale relaxations

S. Mbarek, P. Baroni, L. Noirez

摘要:

研究了无缺口玻璃态聚合物的断裂起始以及玻璃态下零应力下的演化。共焦显微镜观察和自相关方法被用来表征试样的聚甲基丙烯酸甲酯(PMMA)在室温下加载,随后卸载。在零应力松弛过程中的形态和裂纹的位置提交到伸长率高达8%的演变报告和分析。裂纹(纵向裂纹、横向裂纹和银纹)主要发生在离表面10微米厚的层内,而不在本体中延伸。结果表明,应变场继续发展没有应力,它可以描述为一个间歇性的位移场的收缩。相应地,银纹或微空洞的数量在加载后的零应力松弛状态下增加。收缩所涉及的时间尺度是几天的量级,因此报告了迄今为止未知的非常缓慢的弛豫时间尺度。

英文摘要:

Fracture initiation in glassy polymers with no notch is studied together with the evolution at zero stress in the glassy state. Confocal microscopy observations and auto-correlation methods are used to characterize specimens of polymethyl methacrylate (PMMA) loaded at room temperature and subsequently unloaded. The evolution of the morphology and the location of the cracking submitted to elongation rate up to 8% are reported and analyzed during the zero-stress relaxation. The crackling (longitudinal crack, transverse crack and crazes) takes place mainly within a 10micron thickness layer from the surface and does not extend in the bulk. It is shown that the strain field continues to evolve without stress, and that it can be described by an intermittent retraction of the displacement field. Correlatively the number of crazes or of micro-cavities is increasing in the post-loading state at zero-stress relaxation. The timescales involved in the retraction are of the order of several days reporting thus on so far unknown very slow relaxation timescales.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑