Composition-driven structural transitions in Bi1-xCaxFe1-xMnxO3 ceramics prepared by the tartaric acid modified sol-gel technique have been studied to analyze its effect on the magnetic properties of bismuth ferrite (BiFeO3). It was observed that the co-substitution of Ca & Mn at Bi & Fe sites in BiFeO3 (BFO) significantly suppress the impurity phases. The quantitative crystallographic phase analysis has been carried out by double phase Rietveld analysis of all the XRD patterns which indicates the existence of compositional driven crystal structure transformation from rhombohederal (R3c space group, lower crystal symmetry) to the orthorhombic (Pbnm space group, higher crystal symmetry) with the increase in substitution concentration due to excess chemical pressure (lattice strain). Magnetic measurements reveal that co-substituted BFO nanoparticles for x = 0.15 have enhanced remnant magnetization about 14 times that of pure one due to the suppression of cycloid spin structure which could be explained in terms of field induced spin reorientation and weak ferromagnetism. However, at the morphological phase boundary (x = 0.15), the remnant and maximum magnetization at 8 T reaches a maximum which indicates almost broken spin cycloid structure and further increase in substitution results in the reduction of both magnetizations due to the appearance of complete antiferromagnetic ordering in the orthorhombic structure because of the significant contribution from the crystallographic phase of Pbnm space group (as obtained from double phase Rietveld analysis).
Determination of oxygen vacancy limit in Mn substituted YSZ ceramics
采用X射线吸收光谱、发射光谱和直流磁化率等方法对Mn_x(Y_(0.148)Zr_(0.852))_(1-x)O_(2-δ)系列陶瓷进行了系统研究。XAS和XES结果表明,锰的氧化态的变化和Mn离子周围的局部原子环境的逐渐演变的掺杂剂含量增加时,这是由于结构弛豫引起的氧空位的量的增加。磁化率测量表明,Mn 3 O 4沉淀物形成x大于或等于0.1,并使独立的测定的实际量的锰离子溶解在YSZ固溶体。我们表明,锰掺杂到YSZ中产生的氧空位的量被限制为0.19每分子式单位。
Morphotropic Phase Boundary in Sm-Substituted BiFeO3 Ceramics: Local vs Microscopic Approaches
采用溶胶-凝胶法制备了钐取代铁酸铋(BiFeO 3)陶瓷,并利用局部尺度和微观测量技术研究了BiFeO 3陶瓷在准同型相界区域的晶体结构演变。采用X射线衍射分析、透射电镜和扫描电镜、XPS、EDS/EDX实验和压电响应力显微镜研究了Bi_(1-x)Sm_xFeO_3化合物在0.08 < x < 0.2浓度范围内从极性活性菱方相到反极性正交相再到非极性正交相的结构转变。显微技术的研究结果表明,在0.12 < x < 0.15范围内,化合物具有菱方相和反极性正交相共存的两相结构;在0.15 < x < 0.18的化合物中观察到的两相结构状态与反极性正交和非极性正交共存有关。极性正交相局部尺度测量结果表明,由微观测量结果估算的准同型相界浓度范围存在显著差异,证明不同结构相共存导致的浓度范围更宽,并对差异的背景进行了讨论。
Role of charge compensation mechanism on phase formation, dielectric and ferroelectric properties in aliovalent Gd3+ ion modified PbMg1/3Nb2/3O3 ceramics
Relaxor ferroelectric behavior and structural aspects of SrNaBi2Nb3O12 ceramics
采用传统的固相反应法制备了SrNaBi 2Nb 3 O 12粉体。X射线结构研究证实,该相是奥里维利乌斯氧化物家族的三层成员。SrNaBi 2Nb 3 O 12(SNBN)陶瓷表现出典型的弛豫铁电体的特性,与广泛和分散的介电最大值。介电峰温度(Tm)随频率的变化符合Vogel-Fulcher关系。弛豫行为被认为是由A位的阳离子无序引起的。在Tm以上观察到铁电滞回线的收缩。
Si-Substituted MAX Phases and In-Situ Formation of Si-coated MXene Composites via Chlorosilane Etching
Zhejiang Key Laboratory of Data-Driven High-Safety Energy Materials and Applications, Ningbo Key Laboratory of Special Energy Materials and Chemistry, Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences(中国科学院宁波材料技术与工程研究所);University of Chinese Academy of Sciences(中国科学院大学);Qianwan Institute of CNiTECH(中科院宁波新材料技术创新中心)
Structural, dielectric, electrocaloric, and energy storage properties of lead free Ba$_{0.975}$La$_{0.017}$(ZrxTi$_{0.95-x}$)Sn$_{0.05}$O$_3$ (x = 0.05; 0.20) ceramics
Coexistence of Ferroelectric and Relaxor-like Phases in a Multiferroic Solid Solution (1-x)Pb(Fe$_{1/2}$Nb$_{1/2}$)O$_3$-xPbMnO$_3$
Institute of Physics, National Academy of Sciences of Ukraine(乌克兰国家科学院物理研究所);Frantsevich Institute for Problems in Materials Science, National Academy of Sciences of Ukraine(乌克兰国家科学院弗兰采维奇材料科学问题研究所);Ye. O. Paton Institute of Materials Science and Welding, National Technical University of Ukraine “Igor Sikorsky Kyiv Polytechnic Institute”(乌克兰国立技术大学“伊戈尔·西科尔斯基基辅理工学院”叶·奥·帕顿材料科学与焊接研究所)
Nucleation of Al Nanocrystals in Solute-Substituted Al Metallic Glasses I: Structural characterization
高Al含量金属玻璃中的一次晶化是由内部结构类似于面心立方Al的纳米尺度区域驱动的。通过比较涨落电子显微镜(FEM)数据和FEM模拟的面心立方Al团簇在致密随机堆积基质中的分布,提取Al 88 Y 7 Fe 5基础玻璃和Al含量为1 at.%的玻璃中有序区域的直径和体积分数Cu替代Y或Al。纳米晶体的尺寸和密度作为等温退火时间的函数,对于相同的合金进行测量。在等温退火条件下,晶相的体积分数增加,相变不是单纯的晶粒粗化,而是晶相的体积分数低于淬火态样品中有序区的体积分数,因此并非所有有序区都起到晶核的作用。合金化有序区域的直径和体积分数的变化与结晶温度、成核速率和结晶密度的变化相关。没有观察到相分离的证据,相似组成的分子动力学淬火结构模型的FEM模拟没有显示实验中观察到的特征。
Local structural origins of the distinct electronic properties of Nb-substituted SrTiO$_3$ and BaTi$O_3$
在钙钛矿SrTiO $_3$中的Ti位点上接近或小于10%的Nb取代导致金属行为,这与在BaTiO $_3$中所看到的相反。由于两种材料的结构和电子数几乎相同,低取代的不同基态一直是一个长期存在的难题。在这里,我们从平均和局部结构的中子研究中发现,我们认为这些微妙而关键的差异支撑着这些迷人材料中独特的电子特性。而SrTi $_{0.875}$ Nb_ ${0.125}$ O $_3$在15 K下具有畸变的非立方结构,结构中的BO $_6$八面体是规则的。另一方面,BaTi $_{0.875}$ Nb $_{0.125}$ O $_3$显示出局部阳离子偏心同时保持立方结构的证据。
Structural, magnetic, and optical properties of zinc- and copper- substituted nickel ferrite nanocrystals
铁氧体纳米晶由于其丰富的物理性质而成为人们感兴趣的材料。在这里,我们将掺杂剂Zn和Cu添加到镍铁氧体纳米晶体Ni 1-xMxFe 2 O 4(0<=x<=1,M{ \in }{Cu,Zn})中,并表征样品的相关性质如何相应地改变。基本上,这些掺杂导致Fe+3离子重排到两个预先存在的八面体和四面体位置。事实上,这,我们表明,诱导相关的磁性掺杂样品。在Cu掺杂的情况下,Jahn-Teller效应也出现了,我们通过样品的FTIR光谱来识别。此外,我们发现掺杂样品的晶格参数增加,以及掺杂样品的超顺磁性行为,而Jahn-Teller效应排除了CuFe 2 O 4纳米晶体中类似的行为。采用室温光致发光法研究了Zn和Cu掺杂对镍铁氧体纳米晶光学性质的影响。
Structural, Dielectric, and Electrical Transport Properties of Al3+ Substituted Nanocrystalline Ni-Cu Spinel Ferrites Prepared Through the Sol-Gel Route
Temperature Dependent Magnetic and Structural Properties of Al Substituted Nanostructured Ferrites with Large Coercive Fields
University of Genoa(热那亚大学);Uppsala University(乌普萨拉大学);Lomonosov Moscow State University(莫斯科罗蒙诺索夫国立大学);Le Mans Université(勒芒大学);Nuclear Physics Institute of the CAS(捷克科学院核物理研究所);CNR-SPIN(国家研究中心自旋物理研究所);Università Ca’ Foscari Venezia(威尼斯卡福斯卡里大学)
Magnetic, Optoelectronic, and Rietveld refined structural properties of Al3+ substituted nanocrystalline Ni-Cu spinel ferrites: An experimental and DFT based study