arXiv 1301.4756cond-mat.mtrl-sci
收藏

TeO2对草酸盐前驱体法制备CaCu3Ti4O12陶瓷介电性能的影响

Effect of TeO2 addition on the dielectric properties of CaCu3Ti4O12 ceramics derived from the oxalate precursor route

P. Thomas, K. B. R. Varma

摘要:

钙钛矿结构的CaCu3Ti4O12(CCTO)陶瓷由于其巨大的介电常数而受到广泛关注。但是,它在室温下具有高tan δ(在1kHz时为0.1),需要将其最小化到实际应用的水平。因此,TeO2这是一个很好的玻璃形成者已被故意添加到CCTO纳米陶瓷(来自草酸盐前体路线),以探索降低介电损耗,同时保持高介电常数的可能性。采用X射线衍射、扫描电子显微镜、能谱仪、阻抗分析仪等测试手段对纯CTO和添加TeO2的陶瓷的结构、形貌和介电性能进行了研究。对于2.0wt%TeO2添加陶瓷,有一个显着的差异,在微观结构特征相比,纯的CTO陶瓷。该样品表现出高达7387@10KHz的介电常数值和0.037@10kHz的低介电损耗值,这可以用于高频电容器应用。

英文摘要:

CaCu3Ti4O12 (CCTO) ceramics which has perovskite structure gained considerable attention due to its giant permittivity. But, it has high tan δ (0.1 at 1kHz) at room temperature, which needs to be minimised to the level of practical applications. Hence, TeO2 which is a good glass former has been deliberately added to CCTO nano ceramic (derived from the oxalate precursor route) to explore the possibility of reducing the dielectric loss while maintaining the high permittivity. The structural, morphological and dielectric properties of the pure CCTO and TeO2 added ceramics were studied using X-ray diffraction, Scanning Electron Microscope along with Energy Dispersive X-ray Analysis (EDX), spectroscopy and Impedance analyzer. For the 2.0 wt % TeO2 added ceramics, there is a remarkable difference in the microstructural features as compared to that of pure CCTO ceramics. This sample exhibited permittivity values as high as 7387 @ 10 KHz and low dielectric loss value of 0.037 @ 10 kHz, which can be exploited for the high frequency capacitors application.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑