arXivDaily arXiv每日学术速递 周一至周五更新
arXiv 1011.4458cond-mat.mtrl-sci
收藏

铁电体中外延应变的微调:DyScO3上的PbxSr(1-x)TiO3

Fine tuning epitaxial strain in ferroelectrics: PbxSr(1-x)TiO3 on DyScO3

Gijsbert Rispens, Jeroen A. Heuver, Beatriz Noheda

摘要:

外延应变可以用来改变铁电薄膜的性能。从实验的角度来看,挑战在于微调应变的大小。我们说明如何,通过使用组合物和衬底的合适的组合,可以以连续的方式控制外延应变的大小。用Devonshire-Landau方法计算了在(110)-DyScO 3上外延生长的PbxSr 1-xTiO 3薄膜的相图。预测面内和面外取向铁电相之间的边界发生在$x \approx$ 0.8。用分子束外延法生长的一系列PbxSr_(1-x)TiO_3薄膜与所提出的相图符合得很好

英文摘要:

Epitaxial strain can be used to modify the properties of ferroelectric thin films. From the experimental viewpoint, the challenge is to fine-tune the magnitude of the strain. We illustrate how, by using a suitable combination of composition and substrate, the magnitude of the epitaxial strain can be controlled in a continuous manner. The phase diagram of PbxSr1-xTiO3 films grown epitaxially on (110)-DyScO3 is calculated using a Devonshire-Landau approach. A boundary between in-plane and out-of-plane oriented ferroelectric phases is predicted to take place at $x \approx$ 0.8. A series of PbxSr1-xTiO3 films grown by MBE show good agreement with the proposed phase diagram

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑