arXivDaily arXiv每日学术速递 周一至周五更新
arXiv 0908.1215cond-mat.mtrl-sci
收藏

具有Heusler合金Co2FeAl铁磁层的合成反铁磁体

Synthetic antiferromagnet with Heusler alloy Co2FeAl ferromagnetic layers

X. G. Xu, D. L. Zhang, X. Q. Li, J. Bao, Y. Jiang

摘要:

采用Heusler合金Co2 FeAl作为Co2 FeAl/Ru/Co2 FeAl合成反铁磁结构的铁磁层。实验结果表明,Ru层厚度为0.45 nm时,结构呈现强的反铁磁耦合,在150 oC退火1 h后仍能保持强的反铁磁耦合。该结构在室温下具有425 emu/cc的非常低的饱和磁化强度Ms、4.3Oe的低开关场Hsw和5257 Oe的高饱和场Hs,这有利于应用于高密度磁读取头或其它磁存储器件。XRD分析表明,Co2 FeAl薄膜为B2相。因此,Heusler合金可用于制备SyAF,并有可能制备具有更好磁开关特性和高磁阻的“全Heusler”自旋阀或磁隧道结。

英文摘要:

Heusler alloy Co2FeAl was employed as ferromagnetic layers in Co2FeAl/Ru/Co2FeAl synthetic antiferromagnet structures. The experimental results show that the structure with a Ru thickness of 0.45 nm takes on strongly antiferromagnetic coupling, which maintains up to 150 oC annealing for 1 hour. The structure has a very low saturation magnetization Ms of 425 emu/cc, a low switching field Hsw of 4.3 Oe and a high saturation field Hs of 5257 Oe at room temperature, which are favorable for application in ultrahigh density magnetic read heads or other magnetic memory devices. XRD study testifies that the as-deposited Co2FeAl film is in B2 phase. Therefore Heusler alloys can be used to fabricate SyAF and it is possible to make "all-Heusler" spin-valves or magnetic tunneling junctions with better magnetic switching properties and high magnetoresistance.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑