CoSe $_2$ O $_5$具有由沿着c轴延伸的边缘共享的CoO $_6$八面体的Z字形链组成的晶体结构,其中链由Se $_2$ O $_5^{2-}$单元分开。磁化率测量表明,在8.5 K的过渡到有序状态。我们在这里调查的性质,这种磁有序使用磁化强度和比热测量,除了粉末中子衍射。一个过渡到远程反铁磁秩序被发现低于$T_N$ = 8.5 K的磁化率测量和磁布拉格反射,与传播矢量$\mathbf{k}$ = 0。磁结构表明,磁矩垂直于c轴排列,但自旋相对于a轴交替倾斜,分别为$+8^\circ$和$-8^\circ$。有趣的是,低场磁化率并没有表现出预期的尖点行为预期的良好有序的反铁磁体。当磁化率是在10 kOe场下的场冷却条件下获得的,通常预期的反铁磁有序下降。低温下的热容量测量表明存在间隙行为,间隙为6.5 K。
英文摘要:
CoSe$_2$O$_5$ has a crystal structure consisting of zig-zag chains of edge shared CoO$_6$ octahedra running along the c axis, with the chains separated by Se$_2$O$_5^{2-}$ units. Magnetic susceptibility measurements indicate a transition at 8.5 K to an ordered state. We investigate here the nature of this magnetic ordering using magnetization and specific heat measurements in addition to powder neuttron diffraction. A transition to long-range antiferromagnetic order is found below $T_N$ = 8.5 K as identified by magnetic susceptibility measurements and magnetic Bragg reflections, with a propagation vector $\mathbf{k}$ = 0. The magnetic structure shows that the moments align perpendicular to the c-axis, but with the spins canting with respect to the a axis by, alternately, $+8^\circ$ and $-8^\circ$. Interestingly, the low-field magnetic susceptibility does not show the anticipated cusp-like behavior expected for a well-ordered antiferromagnet. When the susceptibility is acquired under field-cooling conditions under a 10 kOe field, the the usual downturn expected for antiferromagnetic ordering is obtained. Heat capacity measurements at low temperatures indicate the presence of gapped behavior with a gap of 6.5 K.
Magnetic-field and pressure phase diagram of the triangular lattice antiferromagnet CsCuCl$_3$ clarified by magnetic susceptibility measured with a proximity detector oscillator
Effects of hydrostatic pressure on the magnetic susceptibility of ruthenium oxide Sr3Ru2O7: Evidence for pressure-enhanced antiferromagnetic instability
Single Crystal Growth, Crystallography, Magnetic Susceptibility, Heat Capacity, and Thermal Expansion of the Antiferromagnetic S = 1 Chain Compound CaV2O4
Long-Time Magnetic Relaxation in Antiferromagnetic Topological Material EuCd$_2$As$_2$
磁性拓扑材料由于其拓扑结构与磁性的相关性而受到人们的广泛关注。最近的研究表明EuCd $_2$ As $_2$是一种反铁磁拓扑材料。通过对EuCd $_2$ As $_2$的磁、电、热性质的测量,发现了EuCd的磁化率的长时间弛豫。发现在5 K下的(001)面内磁化率在$\sim$ 14小时的时间内连续增加直到$\sim$ 10%。磁弛豫是各向异性的,并且强烈地依赖于温度和所施加的磁场。这些结果将激发进一步的理论和实验研究,以了解弛豫过程的起源及其对磁性拓扑材料的电子结构和物理性质的影响。
Signature of spin liquid state in a frustrated 3D antiferromagnet
Indian Institute of Technology Madras(印度马德拉斯理工学院);ISIS Facility, Rutherford Appleton Laboratory(卢瑟福阿普尔顿实验室ISIS设施);R. B. College (A Constituent Unit of Lalit Narayan Mithila University, Darbhanga)(R.B.学院(拉尔·纳亚南·米提拉大学达班加 constituent unit));University of Johannesburg(约翰内斯堡大学);Laboratoire Léon Brillouin, CEA, CNRS, Université Paris-Saclay(莱昂·布里渊实验室,法国原子能和替代能源委员会,法国国家科学研究中心,巴黎萨克雷大学)
Structure and magnetic properties of the $S=3/2$ zigzag spin chain antiferromagnet BaCoTe$_2$O$_7$
报道了$S=3/2$曲折自旋链化合物BaCoTe $_2$ O $_7$的结构和磁性研究。中子衍射测量表明BaCoTe $_2$ O $_7$在2 K时属于非中心对称空间群$Ama2$,具有倾斜的$\uparrow\uparrow\downarrow\downarrow$自旋结构和$1.89(2)μ_B$的磁矩大小.在$T_N=6.2$ K下,磁化率和比热测量产生反铁磁相变.通过对磁化率的拟合,得到了负的居里-外斯温度$Θ_{CW}=-74.7(2)$ K和经验阻挫参数$f=|Θ_\text{CW}|/T_\text{N}\approx12$,表明反铁磁相互作用和强的磁阻挫。通过紫外-可见吸收光谱和第一性原理计算,间接带隙为2.68(2)eV。我们认为BaCoTePDMATHABMN O $_7$的锯齿形自旋链可能通过交换伸缩机制引起极化的变化。