强塑性形变纳米结构FeAuPd合金的分解过程
Decomposition process in a FeAuPd alloy nanostructured by severe plastic deformation
摘要:
研究了Fe_(50)Au_(25)Pd_(25)(at.%)经过剧烈塑性形变加工的合金。用X射线衍射和透射电子显微镜观察相的特征和显微结构。在$450 ^{circ}\mathrm{C}$中均匀化和时效的粗晶合金中,bcc结构的α-Fe和fcc结构的AuPd相在fcc结构的过饱和固溶体中形核,并通过不连续的析出过程长大,形成典型的片层组织。高压扭转使FeAuPd合金的晶粒尺寸减小到50 ~ 100 nm。在$450 ^{circ}\mathrm{C}$下时效,这种纳米结构导致固溶体分解成等轴显微结构。在时效过程中,晶粒生长非常有限,晶粒尺寸保持在100 nm以下。具有不同晶体结构的两相(bcc α-Fe和fcc AuPd)和纳米级晶粒尺寸的组合导致合金的显著硬化
英文摘要:
The decomposition process mechanisms have been investigated in a Fe50Au25Pd25 (at.%) alloy processed by severe plastic deformation. Phases were characterized by X-ray diffraction and microstructures were observed using transmission electron microscopy. In the coarse grain alloy homogenized and aged at $450 ^{circ}\mathrm{C}$, the bcc α-Fe and fcc AuPd phases nucleate in the fcc supersaturated solid solution and grow by a discontinuous precipitation process resulting in a typical lamellar structure. The grain size of the homogenized FeAuPd alloy was reduced in a range of 50 to 100nm by high pressure torsion. Aging at $450 ^{circ}\mathrm{C}$ this nanostructure leads to the decomposition of the solid solution into an equi-axed microstructure. The grain growth is very limited during aging and the grain size remains under 100nm. The combination of two phases with different crystallographic structures (bcc α-Fe and fcc AuPd) and of the nanoscaled grain size gives rise to a significant hardening of the alloy
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。