20 MeV电子辐照TF-1和PbWO$_4$晶体的辐射损伤

Radiation Damage of TF-1 and PbWO$_4$ Crystals with 20 MeV Electrons

A. I. Alikhanyan National Science Laboratory (Yerevan Physice Institute) foundation(阿·伊·阿里哈尼扬国家科学实验室(叶里温物理研究所)基金会)
Hamlet G. Mkrtchyan, Arthur H. Mkrtchyan, Vardan H. Tadevosyan, Hrachya H. Marukyan, Argine S. Hakobyan, Ashot S. Hakobyan, Arthur A. Hoghmrtsyan, Diana G. Khur… 展开作者

Hamlet G. Mkrtchyan, Arthur H. Mkrtchyan, Vardan H. Tadevosyan, Hrachya H. Marukyan, Argine S. Hakobyan, Ashot S. Hakobyan, Arthur A. Hoghmrtsyan, Diana G. Khurshudyan, Nina N. Prazyan, Albert H. Shahinyan, Adelina S. Stepanyan, Lusine R. Vahradyan

AI总结:

利用20 MeV电子束研究TF-1铅玻璃和PbWO$_4$晶体的辐射硬度,发现TF-1光学性能严重退化,而PbWO$_4$辐射硬度高数十倍,且退火可恢复透射率。

摘要:

我们利用AANL的LUE-75直线加速器产生的20 MeV电子束,研究了两种晶体(铅玻璃TF-1和钨酸铅PbWO$_4$)的辐射硬度。在辐照前后以及热退火后,测量了晶体在200-1000 nm波长范围内的透射率。辐照分两个阶段进行。首先,两种晶体均以0.125 μA的束流辐照,总曝光时间720 s,吸收$5.6 \ imes 10^{14}$个电子。观察到该辐射量导致TF-1光学性能严重退化,而对PbWO$_4$的影响可忽略不计(其辐射硬度比TF-1高数十倍)。第二阶段仅对PbWO$_4$晶体进行辐照,束流0.28 μA,曝光时间1200 s,额外吸收$2.1 \ imes 10^{15}$个电子,仍未观察到显著影响。在160至250°C温度范围内进行等时热退火,持续10-12小时。退火晶体的透射率随退火温度和时间的增加而提高。

英文摘要:

We studied the radiation hardness of two types of crystals, lead glass TF-1 and lead tungstate PbWO$_4$, using a 20 MeV electron beam from the LUE-75 linear accelerator at AANL. The transmittance of the crystals in the wavelength range of 200-1000 nm was measured before and after irradiation, and after thermal annealing. % The irradiation was performed in two stages. First, both crystals were irradiated with beam current of 0.125 $μ$A, each for a total exposure time of 720 s and absorbing $5.6 \times 10^{14}~e^-$. % Strong degradation of the optical properties of TF-1 caused by this amount of radiation was observed, while the effect on PbWO$_4$ was negligible (it is a few tens of times radiation harder than TF-1). % In the second stage, only the PbWO$_4$ crystal was exposed to radiation, with a beam current of 0.28 $μ$A and an exposure time of 1200 s, absorbing an additional $2.1 \times 10^{15}e^-$, still no notable effect. % Thermal annealing was performed in the temperature range of 160 to 250$^\circ$C (isochronal) for 10-12 hours. The transmittance of the annealed crystals increased with the annealing temperature and time.