arXivDaily arXiv每日学术速递 周一至周五更新
感恩节,周五至周末无更新,大家顺遂。周一再来吧
arXiv 2605.13611cond-mat.mtrl-sci
收藏

La₀.₆Sr₀.₄Fe₁₋ₓCoₓO₃纳米结构的磁卡效应

Magnetocaloric Effect in Nanostructured $La_{0.6}Sr_{0.4}Fe_{1-x}Co_{x}O_3$

Centro Atómico Constituyentes, CNEA(阿根廷原子能委员会)

Fabiana N. Morales Alvarez, Mariano Quintero, Joaquín Sacanell

AI总结:

研究了La₀.₆Sr₀.₄Fe₁₋ₓCoₓO₃纳米结构的磁卡效应,通过聚合物膜制备不同Co含量的样品,发现Co掺杂增强铁磁耦合,提高磁化率和居里温度,最大熵变达1.13 J/(kg K)。

摘要:

本文系统研究了La₀.₆Sr₀.₄Fe₁₋ₓCoₓO₃纳米结构系列(x=0, 0.2, 0.5, 0.8, 1.0)的磁卡效应,采用聚合物膜孔径为200 nm和800 nm的渗透法合成。所有样品在1000°C煅烧。X射线衍射表征证实形成单相钙钛矿,具有畸变的菱形十二面体对称性,无二次相。扫描电子显微镜分析显示,随着Co含量增加,颗粒从较小变大,纳米管从薄变厚。磁测量显示阳离子掺杂增强铁磁耦合,提高饱和磁化率(MS)和居里温度(TC)。通过麦克斯韦关系确定的磁卡特性,在3 T磁场下,x=1样品的最大熵变达1.13 J/(kg K)。这些结果表明,Co掺杂和可控纳米结构的结合有效优化了磁卡响应。

英文摘要:

This work presents a systematic study of the magnetocaloric effect in the nanostructured perovskite series $La_{0.6}Sr_{0.4}Fe_{1-x}Co_{x}O_3$ (x = 0, 0.2, 0.5, 0.8, and 1.0), synthesized by a pore-wetting method using polymeric membranes with pore diameters of 200 nm and 800 nm. All samples were calcined at 1000°C. Structural characterization was made by X-ray diffraction and confirmed the formation of a single-phase perovskite with distorted rhombohedral symmetry, without detectable secondary phases. We observed significant influence of substitution of Fe by Co on the morphology, as the analysis by scanning electron microscopy revealed a clear evolution from smaller to larger particles and from thin to thicker nanotubes, as the Co content increased. Magnetic measurements showed that the cationic substitution enhances ferromagnetic coupling, increasing both the saturation magnetization (MS) and the Curie temperature (TC). The magnetocaloric properties, determined through the Maxwell relations, exhibit a maximum entropy change of 1.13 J/(kg K) under an applied field of 3 T for the sample with x = 1. These results demonstrate that the combination of Co doping and controlled nanostructuring effectively optimizes the magnetocaloric response.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑