短时球磨对R5(Si,Ge)4,R =Gd和Tb磁热材料的影响

Influence of short time milling in R5(Si,Ge)4, R =Gd and Tb, magnetocaloric materials

A. L. Pires, J. H. Belo, J. Turcaud, G. N. P. Oliveira, J. P. Araújo, A. Berenov, L. F. Cohen, A. M. L. Lopes, A. M. Pereira

摘要:

研究了短球磨时间对R5(Si,Ge)4 R =Gd,Tb磁热材料性能的影响。特别地,研究了研磨对原子结构、颗粒尺寸和形态、磁性和磁热效应的影响。在短的研磨时间(< 2.5h)下,实现了Gd5Si1.3Ge2.7和Tb5Si2Ge2颗粒尺寸减小至约3.5DSm。对于这两种组合物的主要差异是研磨效应的结构和磁性转变的耦合的后果。在Gd5Si1.3Ge2.7的情况下,二阶相变出现在高温球磨的结果。因此,在研磨150分钟后,磁热效应降低35%。有趣的是,在Tb5Si2Ge2中观察到相反的效果,其中磁热效应增加了23%,这是由研磨过程促进的内部应变引起的磁性和结构转变之间的耦合增强驱动的。

英文摘要:

The effect of the short milling times on R5(Si,Ge)4 R =Gd, Tb magnetocaloric material properties was investigated. In particular, the effect of milling on atomic structure, particles size and morphology, magnetic, and magnetocaloric effect was studied. With short milling times (< 2.5h), a reduction of the Gd5Si1.3Ge2.7 and Tb5Si2Ge2 particles size was achieved down to approximately 3.5 DSm. For both compositions the main differences are a consequence of the milling effect on the coupling of the structural and magnetic transitions. In the Gd5Si1.3Ge2.7 case, a second-order phase transition emerges at high temperatures as a result of ball milling. Consequently, there is a decrease in the magnetocaloric effect of 35% after 150 minutes of milling. Interestingly, an opposite effect is observed in Tb5Si2Ge2 where a 23% increase of the magnetocaloric effect was achieved, driven by the enhancement of the coupling between magnetic and structural transitions arising from internal strain promoted by the milling process.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑