arXiv 2312.04409cond-mat.mtrl-sci
收藏

通过界面工程调控Re(0001)上Co与4d过渡金属原子双层膜的磁相互作用

Tuning magnetic interactions of Co and 4$d$ transition-metal atomic bilayers on Re(0001) via interface engineering

Souvik Paul, Stefan Heinze

AI总结:

该研究利用DFT和有效自旋哈密顿量,揭示Re(0001)上Co与Rh、Pd、Ru双层膜的组成及堆叠方式对交换、DMI和MAE的显著调控作用。

摘要:

我们采用从头算密度泛函理论(DFT),系统研究了Re(0001)表面由4d过渡金属层(Rh、Pd和Ru)与Co层构成的原子双层膜的电子结构和磁学性质。DFT计算揭示了双层膜组成及其堆叠顺序对磁基态和磁相互作用的影响。我们通过将总能量映射到一个有效自旋哈密顿量来获得磁相互作用,该哈密顿量包含交换相互作用、Dzyaloshinskii-Moriya相互作用(DMI)以及磁晶各向异性能(MAE)。我们观察到,双层膜组成和覆盖层对称性的变化会引起双层膜杂化的显著改变,从而导致磁相互作用发生显著变化。在所有考虑的体系中,最近邻交换相互作用均为铁磁性,但其数值差异最大可达5倍。有效最近邻DMI常数在所研究的薄膜中表现出符号变化,分别有利于右手(顺时针)或左手(逆时针)摆线自旋螺旋。不同薄膜之间DMI数值的变化最大可达27倍。对于大多数体系,MAE有利于面外易磁化轴;但对于Re(0001)上的hcp-Co/Rh和hcp-Co/Ru双层膜,MAE更倾向于面内磁化轴。MAE的大小从约0.1 meV/Co原子的较小值变化到Co/Pd双层膜的约2 meV/Co原子。对于Co层邻近真空的薄膜,自旋螺旋能量色散曲线在铁磁态附近上升得相当快,这表明存在较大的有效交换常数,可稳定Re(0001)上Co/4d双层膜的铁磁基态。

英文摘要:

Employing $\textit{ab-initio}$ density functional theory (DFT), we performed a systematic investigation of the electronic structures and the magnetic properties of atomic bilayers composed of a 4$d$ transition-metal layer (Rh, Pd and Ru) and a Co layer on the Re(0001) surface. Our DFT calculations reveal the influence of the bilayer composition and their stacking sequence on the magnetic ground state and magnetic interactions. We obtain the magnetic interactions by mapping the total energies onto an effective spin Hamiltonian which contains the exchange interaction and the Dzyaloshinskii-Moriya interaction (DMI) as well as the magnetocrystalline anisotropy energy (MAE). We observe noticeable changes in bilayer hybridization due to variation in bilayer composition and overlayer symmetry, leading to significant variation in magnetic interactions. In all considered systems, the nearest-neighbor exchange interaction is ferromagnetic, however, the value varies by up to a factor of 5. The effective, nearest-neighbor DMI constant exhibits variation in sign over the films considered, favoring either right- (clockwise) or left-handed (anticlockwise) cycloidal spin spirals. The value of the DMI changes by up to a factor of 27 among the films. For most of the systems, the MAE favors an out-of-plane easy magnetization axis, however, for hcp-Co/Rh and hcp-Co/Ru bilayers on Re(0001), it prefers an in-plane magnetization axis. The magnitude of the MAE varies from a small value of about 0.1 meV/Co atom up to about 2 meV/Co atom for Co/Pd bilayers. The spin spiral energy dispersion curve rises quite quickly close to the ferromagnetic state for films in which the Co layer is adjacent to the vacuum indicating a large effective exchange constant which stabilizes a ferromagnetic ground state in Co/$4d$ bilayers on Re(0001).

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑