Fe-Mn-Al-C低密度钢时效过程中的微观组织演变与力学行为

Microstructure evolution and mechanical behavior of Fe-Mn-Al-C low-density steel upon aging

Alexandros Banis, Andrea Gomez, Vitaliy Bliznuk, Aniruddha Dutta, Ilchat Sabirov, Roumen H. Petrov

AI总结:

本研究探究Fe-28Mn-9Al-1C低密度钢不同时效条件下的微观组织演变,揭示k-碳化物的形核生长规律,确定550℃时效8小时为最优工艺,实现了高强度与高塑性的良好匹配。

摘要:

本研究聚焦于成分为Fe-28Mn-9Al-1C的高强度低密度钢在不同时效条件下的微观组织演变。该钢经热轧后,未进行任何固溶处理直接淬火,随后在不同条件下进行时效处理。研究采用扫描电子显微镜、电子背散射衍射和透射电子显微镜对样品的微观组织进行了表征。时效处理会促使一种名为k-碳化物(k-carbide)的有序面心立方L1₂相形成。本研究旨在定性和定量表征不同时效条件下这些k-碳化物的形成与生长规律,随后尝试将该相的体积分数和尺寸与钢的拉伸性能关联起来,以确定能实现强度与塑性良好匹配的最优时效条件。研究发现,k-碳化物首先通过奥氏体晶粒内部铝和锰的浓度波动在晶内形核,随后通过调幅分解过程与基体保持共格关系长大。在此过程中,钢的强度和硬度不断提升,同时保持了较高的延伸率。在550℃时效8小时的条件下,钢获得了最佳的强塑性匹配,其抗拉强度最高达1157 MPa,总延伸率为51%。当时效温度升高、时效时间延长时,k-碳化物开始在晶界形成,失去与基体的共格关系,会严重降低钢的硬度和强度。本研究还探讨了变形过程中碳化物的剪切机制。

英文摘要:

This study focuses on the microstructure's evolution upon different aging conditions of a high-strength low-density steel with a composition of Fe-28Mn-9Al-1C. The steel is hot-rolled, subsequently quenched without any solution treatment, and then aged under different conditions. The microstructure of the samples was studied by means of Scanning Electron Microscopy, Electron Backscatter Diffraction, and Transmission Electron Microscopy. The aging treatment leads to the formation of an ordered face-centered cubic L12 phase named k-carbide. This study aims to characterize the formation and growth of these k-carbides qualitatively and quantitatively under different aging conditions. Then, an effort is made to relate the fraction and size of this phase with the tensile properties of the steel to determine the optimal aging conditions that will lead to a good combination of strength and ductility. It has been found that the k-carbides start to form intragranularly through concentration fluctuations of aluminum and manganese inside the austenite grain. Then, with the process of spinodal decomposition, they grow in size coherently with the matrix. During this process, the strength and hardness of the steel increase while maintaining a relatively high elongation. The best combination of high strength and ductility was achieved at the aging condition of 8 h at 550 degrees Celsius with an ultimate tensile strength up to 1157 MPa and total elongation of 51%. Increasing the aging temperature and time, k-carbides start to form intergranularly, lose their coherency with the matrix and severely compromise the hardness and strength. The shearing of the carbides during deformation is also studied.