贫Mg-Zn-Ca合金中的析出

Precipitation in lean Mg-Zn-Ca alloys

R. E. Schaublin, M. Becker, M. Cihova, S. S. A. Gerstl, D. Deiana, C. Hebert, S. Pogatscher, P. J. Uggowitzer, J. F. Loffler

摘要:

虽然贫Mg-Zn-Ca合金是用于临时植入物的有前途的材料,但Zn和Ca的影响仍存在问题。在这种情况下,在Mg-1.5Zn-0.25Ca(ZX 20,以重量%计)中的沉淀物在从大约室温线性加热到400 ℃时,特别关注于有争议的三元沉淀相。差示扫描量热法(DSC)在125、250和320 ℃观察到三个放热峰.在这些峰(205,260和350 C)的末端的微观结构,探测在多尺度相关的方法,使用原子探针断层扫描(APT)和透射电子显微镜(TEM)。在205 C下,APT分析显示富Ca、富Zn和富Zn-Ca团簇的尺寸约为3 nm,数密度为5.7 x 10^23 m^-3。在260 ℃下,APT和TEM显示出尺寸约为8 nm、数密度为1.3 x 10^23 m^-3的单层富Zn-Ca Guinier-Preston(GP)区。在350 ℃下,存在尺寸约为50 nm的较大的、高度共格的细长沉淀物,数量密度较低,并且有两种类型:二元Mg 2Ca沉淀物或数量较少的三元Ca 2 Mg 6 Zn 3沉淀物,如从扫描TEM-基能量色散X射线光谱(EDS)和TEM中的纳米衍射推断的。通过维氏硬度测试探测的最高硬化与125 C DSC峰的末端相关,因此与GP区相关,其优于由纳米级簇和较大的金属间化合物颗粒诱导的硬化。将线性加热时ZX 20中的沉淀与在330 ℃下热挤压诱导的沉淀进行比较。在这里,三元沉淀物的数量超过二元沉淀物,并且更大、不连贯且数量密度低得多。它们是明确的六方晶系Ca 2 Mg 5 Zn 5,推断原子分辨EDS映射和扫描TEM成像,并支持模拟。讨论了贫Mg-Zn-Ca合金中析出相的复杂性及其动力学途径。

英文摘要:

While lean Mg-Zn-Ca alloys are promising materials for temporary implants, questions remain on the impact of Zn and Ca. In this context, the precipitation in Mg-1.5Zn-0.25Ca (ZX20, in wt.%) was investigated upon linear heating from about room temperature to 400 C, with a particular focus on the debated ternary precipitate phase. Three exothermic differential scanning calorimetry (DSC) peaks were observed at 125, 250 and 320 C. The microstructure at the end of these peaks (205, 260 and 350 C) was probed in a multiscale correlative approach using atom probe tomography (APT) and transmission electron microscopy (TEM). At 205 C, APT analysis revealed Ca-rich, Zn-rich and Zn-Ca-rich clusters of about 3 nm in size and with a number density of 5.7 x 10^23 m^-3. At 260 C, APT and TEM showed mono-layered Zn-Ca-rich Guinier-Preston (GP) zones of about 8 nm in size and with a number density of 1.3 x 10^23 m^-3. At 350 C, there are larger, highly coherent elongated precipitates of about 50 nm in size, in a lower number density, and of two types: either binary Mg2Ca precipitates or less numerous ternary Ca2Mg6Zn3 precipitates, as deduced from scanning TEM-based energy dispersive X-ray spectrometry (EDS) and nanodiffraction in TEM. The highest hardening, probed by Vickers testing, relates to the end of the 125 C DSC peak and thus to GP zones, which outperform the hardening induced by the nanoscale clusters and the larger intermetallic particles. Precipitation in ZX20 upon linear heating was compared to the one induced by hot extrusion at 330 C. Here, ternary precipitates outnumber the binary ones and are larger, incoherent, and in a much lower number density. They are unequivocally made of hexagonal Ca2Mg5Zn5, as deduced by atomically resolved EDS mapping and scanning TEM imaging, and supported by simulations. Precipitation complexity of in lean Mg-Zn-Ca alloys and its kinetic path are discussed.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑