尖晶石型CoFe $_2$ O $_4$是一种铁磁绝缘体,其Néel温度超过790 K,并且在块体材料中显示出强的立方磁晶各向异性(MCA)。然而,当在其它材料上生长CoFe $_2$ O $_4$膜时,其磁性能劣化,从而预期在界面区域中形成所谓的磁死层。利用X射线磁性圆二色性(XMCD)研究了Si(111)衬底上生长的CoFe $_2$ O $_4$ /Al $_2$ O $_3$双层膜界面处CoFe $_2$ O $_4$的磁各向异性是如何改变的.我们发现,较薄的CoFe $_2$ O $_4$薄膜具有显着较小的MCA值比散装材料。MCA的减少由先前的研究报道的在$O_h$位点的Co $^{2+}$离子的数量减少来解释[Y. K. Wakabayashi $\textit{et al.}$,Phys. Rev. B $\textbf{96}$,104410(2017)]。
英文摘要:
Spinel-type CoFe$_2$O$_4$ is a ferrimagnetic insulator with the Néel temperature exceeding 790 K, and shows a strong cubic magnetocrystalline anisotropy (MCA) in bulk materials. However, when a CoFe$_2$O$_4$ film is grown on other materials, its magnetic properties are degraded so that so-called magnetically dead layers are expected to be formed in the interfacial region. We investigate how the magnetic anisotropy of CoFe$_2$O$_4$ is modified at the interface of CoFe$_2$O$_4$/Al$_2$O$_3$ bilayers grown on Si(111) using x-ray magnetic circular dichroism (XMCD). We find that the thinner CoFe$_2$O$_4$ films have significantly smaller MCA values than bulk materials. The reduction of MCA is explained by the reduced number of Co$^{2+}$ ions at the $O_h$ site reported by a previous study [Y. K. Wakabayashi $\textit{et al.}$, Phys. Rev. B $\textbf{96}$, 104410 (2017)].
Electronic structure and magnetic properties of magnetically dead layers in epitaxial CoFe2O4/Al2O3/Si(111) films studied by X-ray magnetic circular dichroism
由于CoFe_2 O_4的自旋过滤效应,CoFe_2 O_4/Al_2 O_3双层外延膜有望成为Si中高效的自旋注入器。为了充分利用该系统的潜力,了解磁死层的微观起源在CoFe 2 O 4/Al 2 O3界面是必要的。本文研究了不同厚度的CoFe_2O_4(111)薄膜的晶体结构、电子结构和磁性(厚度d = 1.4,2.3,4,利用软X射线吸收谱(XAS)和X射线磁性圆二色性(XMCD)结合团簇吸收谱(GCD)研究了CoFe_2 O_4(111)/Al_2 O_3(111)/Si(111)外延结构中(10 nm和11 nm)的磁性。模型计算通过XMCD测量的CoFe 2 O 4的磁化强度随着厚度d的减小而逐渐减小,并且最终在d = 1.4nm处清楚地检测到磁死层。磁死层具有磁相互作用的挫折,这是从在300和6 K的磁化强度之间的比较中揭示的。从使用组态相互作用簇模型计算的分析,d的减少导致反尖晶石结构比的减少,并且在八面体位置处的Fe的平均价态也减少。这些结果强烈表明,磁死层在CoFe 2 O 4/Al 2 O3界面起源于各种复杂的网络的超交换相互作用,通过在晶体结构和电子结构的变化。此外,从d = 1.4和2.3 nm之间的磁性能的比较,发现在d = 1.4 nm处的磁死层的亚铁磁顺序通过在其上附加生长0.9 nm厚的CoFe 2 O 4层而恢复。
Contributions of Co and Fe orbitals to Perpendicular Magnetic Anisotropy of MgO/CoFeB Bilayers with Spin-Orbit-Torque-Related (Ta, W, IrMn, and Ti) Underlayers
Magnetoresistance in Hybrid Pt/CoFe2O4 Bilayers Controlled by Competing Spin Accumulation and Interfacial Chemical Reconstruction
纯自旋电流有望成为能量友好的自旋电子学。它们可以由沿着具有大自旋轨道耦合的非磁性金属的电荷流产生。它在其表面产生自旋累积,可由相邻铁磁层的磁化控制。通常使用的顺磁性金属接近铁磁不稳定性,因此磁邻近效应可以有助于观察到的角相关磁阻(ADMR)。由于界面现象支配着金属/铁磁绝缘体异质结构的自旋电导,解开这些不同的贡献是充分理解自旋电流电导的关键。我们在这里报告的X射线吸收和磁性圆二色性(XMCD)在Pt-M和(Co,Fe)-L的吸收边和原子分辨能量损失电子能谱(EELS)的数据Pt/CoFe 2 O 4双层膜CoFe 2 O 4层已被Pt在不同温度下生长。结果表明,ADMR的差异显着,无论是主导的自旋霍尔磁阻(SMR)相关的自旋霍尔效应或各向异性磁阻(AMR)。的XMCD和EELS数据表明,在室温下生长的Pt层不显示任何磁矩,而在较高的温度下生长时,它是磁性的,由于界面Pt-(Co,Fe)合金化。这些结果允许解开自旋积累界面化学重建和定制的角度依赖磁阻。
Anisotropic Band-Split Magnetism in Magnetostrictive CoFe$_2$O$_4$
The University of Manchester(曼彻斯特大学);University of St Andrews(圣安德鲁斯大学);University of Edinburgh(爱丁堡大学);Tohoku University(东北大学);Tokyo Metropolitan University(东京都立大学);Kyoto University(京都大学);Paul Scherrer Institut(保罗谢尔研究所);STFC Rutherford Appleton Laboratory(STC卢瑟福阿普尔顿实验室);Royal Holloway University of London(伦敦皇家霍洛威学院)
Absence of magnetic proximity effects in magnetoresistive Pt/CoFe2O4 hybrid interfaces
在绝缘亚铁磁CoFe 2 O 4(111)外延膜上生长的超薄Pt膜在旋转磁性层的磁化时显示磁阻。我们在这里报告的X射线磁圆二色性(XMCD)记录在Pt-L2,3和Pt-M3边缘。结果表明,Pt磁矩(如果有的话)低于检测限(< 0.001 μ $_B$ /Pt),因此强烈支持CoFe 2 O 4的存在不会诱导Pt中形成磁矩的观点。因此,所观察到的磁阻不能归因于某种接近感生的磁矩在Pt离子和随后的磁场依赖的散射。因此,无论是体(自旋霍尔和逆自旋霍尔效应)或界面(Rashba)自旋轨道相关的影响占主导地位的观察到的磁阻。此外,在(Fe,Co)-L2,3边缘的体磁化强度和XMCD数据的比较表明,在CoFe 2 O 4层中存在一些自旋无序,这可能与所观察到的自旋霍尔磁阻的异常非饱和场依赖性有关。
Systematic study of the electronic structure and the magnetic properties of a few-nm-thick epitaxial (Ni1-xCox)Fe2O4 (x = 0 - 1) layers grown on Al2O3(111)/Si(111) using soft X-ray magnetic circular dichroism: effects of cation distribution
我们研究了外延晶体的电子结构和磁性(Ni 1-xCox)Fe 2 O 4(111)层(x = 0 - 1),厚度d = 1.7 - 5.2 nm,以获得高的反转参数y值,该反转参数y是反转与正向尖晶石结构的比率,因此即使当厚度薄到足以使电子隧穿作为自旋过滤器时也能获得良好的磁性能。我们揭示了晶体学(八面体哦或四面体Td)网站和Fe,Co,Ni阳离子的价态,使用实验软X射线吸收光谱和X射线磁性圆二色光谱和组态相互作用集群模型计算。在所有d =约4 nm的(Ni 1-xCox)Fe 2 O 4层中,所有Ni阳离子占据Ni 2+(Oh)位点,而Co阳离子以恒定的占据率占据三种不同的Co 2+(Oh)、Co 2+(Td)和Co 3+(Oh)位点。根据这些特征,随着x的减小,Fe 3+(Oh)阳离子的占据减少,而Fe 3+(Td)阳离子的占据增加。因此,我们得到了一个系统的y的增加与减少x,并实现了最高的y值为0.91的NiFe 2 O 4层与d = 3.5 nm。从1.7 - 5.2nm的d范围内y和磁化强度的d依赖性来看,在NiFe_2O_4/Al_2O_3界面附近存在磁死层,但与先前报道的CoFe_2O_4层的情况相比,其对磁化强度的影响被显著抑制[Y. K. Wakabayasi等人,Phys. Rev. B 96,104410(2017)],这是由于Ni阳离子的高位点选择性。由于我…
Tuning Structure and Magnetism in Large-Scale 2D Ferromagnet Fe$_3$GeTe$_2$ through Ni Doping
Department of Physics and Astronomy, Uppsala University(乌普萨拉大学物理与天文系);Zernike Institute for Advanced Materials, University of Groningen(格罗宁根大学泽尔尼克先进材料研究所);ALBA Synchrotron Light Facility, CELLS(阿尔巴同步辐射光源设施,CELLS);Helmholtz-Zentrum Dresden-Rossendorf, Institute of Ion Beam Physics and Materials Research(德累斯顿-罗斯多夫亥姆霍兹中心,离子束物理与材料研究所);Departament de Física de la Matéria Condensada, Universitat de Barcelona(巴塞罗那大学凝聚态物理系);Institut de Nanociéncia i Nanotecnologia (IN2UB), Universitat de Barcelona(巴塞罗那大学纳米科学与纳米技术研究所(IN2UB))