Fe5PB2及其含Co和5d元素合金的磁晶各向异性:第一性原理和实验研究

Magnetocrystalline anisotropy of Fe5PB2 and its alloys with Co and 5d elements: a combined first-principles and experimental study

Mirosław Werwiński, Alexander Edström, Ján Rusz, Daniel Hedlund, Klas Gunnarsson, Peter Svedlindh, Johan Cedervall, Martin Sahlberg

摘要:

Fe $_5$ PB $_2$化合物通过Fe和P位点上的各种取代组合的可能性提供可调的磁性。在这里,我们提出了一个综合的计算和实验研究的磁性(Fe $_{1-x}$ Co $_{x}$)$_5$ PB $_2$。在计算上,我们能够探索整个浓度范围,而实际样品仅在0 <= x <= 0.7时获得。计算的磁矩,居里温度,和磁晶各向异性能(MAEs)被发现随Co浓度的增加而减少。钴的替代可以在很宽的范围内调节居里温度,从大约600到零开。由于MAE依赖于费米能级附近的电子结构,本文讨论了Fe $_5$ PB $_2$的费米面几何结构以及k分辨对MAE的贡献。低温下测量一系列的有效各向异性常数(Fe $_{1-x}$ Co $_{x}$)$_5$ PB $_2$样品确定了末端Fe $_5$ PB $_2$组成的最高值0.94 MJ m $^{-3}$,然后随着Co浓度的增加而降低,从而证实了Fe $_5$ PB $_2$的Co合金化不是提高体系MAE的好策略的计算结果。然而,固定自旋矩方法的相对论版本揭示了Fe $_5$ PB $_2$的磁矩减少约25%,产生四倍的MAE增加。此外,(Fe $_{0.95}$ X $_{0.05}$)$_5$ PB $_2$(X = 5个$d$元素)的计算表明,Fe $_5$ PB $_2$掺杂5% W或Re应使MAE翻倍。这些是高度关注的结果,例如,永磁体应用,其中大MAE至关重要。

英文摘要:

The Fe$_5$PB$_2$ compound offers tunable magnetic properties via the possibility of various combinations of substitutions on the Fe and P-sites. Here, we present a combined computational and experimental study of the magnetic properties of (Fe$_{1-x}$Co$_{x}$)$_5$PB$_2$. Computationally, we are able to explore the full concentration range, while the real samples were only obtained for 0 <= x <= 0.7. The calculated magnetic moments, Curie temperatures, and magnetocrystalline anisotropy energies (MAEs) are found to decrease with increasing Co concentration. Co substitution allows for tuning the Curie temperature in a wide range of values, from about six hundred to zero kelvins. As the MAE depends on the electronic structure in the vicinity of Fermi energy, the geometry of the Fermi surface of Fe$_5$PB$_2$ and the k-resolved contributions to the MAE are discussed. Low temperature measurements of an effective anisotropy constant for a series of (Fe$_{1-x}$Co$_{x}$)$_5$PB$_2$ samples determined the highest value of 0.94 MJ m$^{-3}$ for the terminal Fe$_5$PB$_2$ composition, which then decreases with increasing Co concentration, thus confirming the computational result that Co alloying of Fe$_5$PB$_2$ is not a good strategy to increase the MAE of the system. However, the relativistic version of the fixed spin moment method reveals that a reduction in the magnetic moment of Fe$_5$PB$_2$, by about 25%, produces a fourfold increase of the MAE. Furthermore, calculations for (Fe$_{0.95}$X$_{0.05}$)$_5$PB$_2$ (X = 5$d$ element) indicate that 5% doping of Fe$_5$PB$_2$ with W or Re should double the MAE. These are results of high interest for, e.g., permanent magnet applications, where a large MAE is crucial.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑