采用高能球磨法制备了BaMg 2-xCoxFe 16 O27(x = 0.0,1.0和2.0)前驱体粉末,利用X射线衍射仪(XRD)、扫描电镜(SEM)和振动样品磁强计(VSM)研究了化学成分和烧结温度对前驱体粉末结构和磁性能的影响。XRD分析表明,在1300° C烧结时,BaW晶化为纯六角铁氧体相,而在1100° C和1200° C烧结时,BaM晶化为立方尖晶石相。SEM照片显示,随着烧结温度的升高,结构相的结晶程度提高,颗粒尺寸增大。在1300° C下烧结的样品的磁性数据显示,随着Co浓度(x)从0.0增加到2.0,饱和磁化强度从59.44 emu/g增加到72.56 emu/g。矫顽场Hc从x = 0.0时的0.07 kOe下降到x = 1.0时的0.03 kOe,然后增加到x = 2.0时的0.09 kOe。在1300° C下烧结的样品的热磁曲线证实了W型相的存在,并揭示了高于室温的自旋重取向转变。

英文摘要:

Precursor powders of BaMg2-xCoxFe16O27 with (x = 0.0, 1.0, and 2.0) were prepared using high-energy ball milling, and the effects of chemical composition and sintering temperature on the structural and magnetic properties were investigated using x-ray diffractometer (XRD), scanning electron microscopy (SEM), and vibrating sample magnetometry (VSM). XRD patterns of the prepared samples indicated that crystallization of pure BaW hexaferrite phase was achieved at sintering temperature of 1300° C, while BaM and cubic spinel phase intermediate phases were obtained at lower sintering temperatures of 1100° C and 1200° C. SEM images revealed improvement of the crystallization of the structural phases, and growth of the particle size with increasing the sintering temperature. The magnetic data of the samples sintered at 1300° C revealed an increase of the saturation magnetization from 59.44 emu/g to 72.56 emu/g with increasing Co concentration (x) from 0.0 to 2.0. The coercive field Hc decreased from 0.07 kOe at x = 0.0, to 0.03 kOe at x = 1.0, and then increases to 0.09 kOe at x = 2.0. The thermomagnetic curves of the samples sintered at 1300° C confirmed the existence of the W-type phase, and revealed spin reorientation transitions above room temperature.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑