球磨Co-Zn Y型六角铁氧体的结构和穆斯堡尔谱研究
Structural and Mossbauer studies of ball milled Co-Zn Y-type hexaferrites
摘要:
以柠檬酸盐溶胶-凝胶自燃烧法合成的前驱体为原料,制备了Y型六角铁氧体样品Ba 2 ZnxCo 2-xFe 12 O22(x = 0,1和2)。将粉末在1100° C下烧结4小时。利用X射线衍射、扫描电子显微镜和穆斯堡尔谱研究了球磨对样品结构、显微结构和超精细参数的影响。X-射线衍射表明,在所有烧结样品中存在单一的Y型六角铁氧体。该阶段在研磨长达4小时的样品中持续存在。扫描电子显微镜图像表明,颗粒的形状发生了变化,其尺寸在研磨4小时后减小了10倍。室温穆斯堡尔谱的六角铁氧体阐明了分布的各种阳离子在不同的网站的六角铁氧体晶格。超精细领域(BHF)与每个组件被发现几乎呈指数下降,随着研磨时间的增加。超精细场的减少与自旋向上和自旋向下的亚晶格之间的超交换相互作用的减弱有关,这是由于非磁性Zn 2+离子取代Co 2+磁性离子以及研磨样品中的微观结构。
英文摘要:
Y-type hexaferrite samples Ba2ZnxCo2-xFe12O22 with x = 0, 1 and 2 were prepared from precursors synthesized by the citrate sol-gel auto combustion method. The powders were sintered at 1100° C for four hours. X-ray diffraction, scanning electron microscopy and Mössbauer spectroscopy were used to investigate the effect of ball milling on the structure, microstructure and on the hyperfine parameters. X-ray diffraction revealed the presence of a single Y-type hexaferrite in all sintered samples. This phase persisted in samples milled for periods up to four hours. Scanning electron microscopy images indicated that the particles changed shape, and their sizes reduced by a factor of 10 for milling times of four hours. Room temperature Mössbauer spectra of the hexaferrites elucidated the distribution of the various cations at the various sites of the hexaferrite lattice. The hyperfine field (Bhf) associated with each component was found to decrease almost exponentially with increasing milling time. The reduction in hyperfine field was associated with the weakening of the superexchange interactions between the spin-up and spin-down sublattices as a consequence of replacing Co2+ magnetic ions by non-magnetic Zn2+ ions and with the microstructure in the milled samples.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。