arXivDaily arXiv每日学术速递 周一至周五更新
感恩节,周五至周末无更新,大家顺遂。周一再来吧
arXiv 1606.01388quant-phcond-mat.mes-hallcond-mat.mtrl-sciphysics.optics
收藏

金刚石中氦相关色心的产生与表征

Creation and characterization of He-related color centers in diamond

Jacopo Forneris, Andrea Tengattini, Sviatoslav Ditalia Tchernij, Federico Picollo, Alfio Battiato, Paolo Traina, Ivo Degiovanni, Ekaterina Moreva, Giorgio Brida… 展开作者

Jacopo Forneris, Andrea Tengattini, Sviatoslav Ditalia Tchernij, Federico Picollo, Alfio Battiato, Paolo Traina, Ivo Degiovanni, Ekaterina Moreva, Giorgio Brida, Veljko Grilj, Natko Skukan, Milko Jakšić, Marco Genovese, Paolo Olivero

摘要:

金刚石在量子光学、量子信息和量子传感等领域有着广泛的应用前景。因此,制造和表征具有合适的光物理性质的新型发光缺陷对于这些研究领域的进一步发展至关重要。在这项工作中,我们报告的调查,在光致发光(PL)缺陷的形成后,MeV的He注入金刚石。这种色心,以前只报道在电致发光和阴极射线发光制度,表现出两个尖锐的发射线在536.5 nm和560.5 nm,没有显着的声子边带。在10^15-10^17 cm^{-2}注量范围内,上述发射线的PL强度与He注入注量有很强的相关性。在对照样品中未检测到PL发射特征,对照样品即未经辐照或用不同离子种类(H、C)辐照的样品。此外,PL发射线消失的样品,氦注入石墨化阈值以上。因此,PL特征归因于与He杂质相关的金刚石基质中的光学活性缺陷。536.5 nm和560.5 nm发射线的强度作为金刚石衬底的退火温度的函数进行了研究。在高于500°C的温度下退火时观察到发射,代价是同时降低中性空位相关的GR 1发射强度。因此,我们的研究结果表明,发光起源于一个稳定的晶格缺陷的形成。最后,在不同的激光激发波长(即532 nm和405 nm)下的发射进行了研究,目的是获得一个初步的洞察有关的水平在金刚石的能隙的位置。

英文摘要:

Diamond is a promising material for the development of emerging applications in quantum optics, quantum information and quantum sensing. The fabrication and characterization of novel luminescent defects with suitable opto-physical properties is therefore of primary importance for further advances in these research fields. In this work we report on the investigation in the formation of photoluminescent (PL) defects upon MeV He implantation in diamond. Such color centers, previously reported only in electroluminescence and cathodoluminescence regime, exhibited two sharp emission lines at 536.5 nm and 560.5 nm, without significant phonon sidebands. A strong correlation between the PL intensities of the above-mentioned emission lines and the He implantation fluence was found in the 10^15-10^17 cm^{-2} fluence range. The PL emission features were not detected in control samples, i.e. samples that were either unirradiated or irradiated with different ion species (H, C). Moreover, the PL emission lines disappeared in samples that were He-implanted above the graphitization threshold. Therefore, the PL features are attributed to optically active defects in the diamond matrix associated with He impurities. The intensity of the 536.5 nm and 560.5 nm emission lines was investigated as a function of the annealing temperature of the diamond substrate. The emission was observed upon annealing at temperatures higher than 500°C, at the expenses of the concurrently decreasing neutral-vacancy-related GR1 emission intensity. Therefore, our findings indicate that the luminescence originates from the formation of a stable lattice defect. Finally, the emission was investigated under different laser excitations wavelengths (i.e. 532 nm and 405 nm) with the purpose of gaining a preliminary insight about the position of the related levels in the energy gap of diamond.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑