Charge transfer plays the central role in chemisorption and chemical reactions at metal surfaces. The Somorjai group in Nano. Lett. {\bf 9}, 3930 (2009) has reported a chemicurrent, a flux of charge carriers in response to $\mathrm{H_2}$ oxidation by $\mathrm{O_2}$ into $\mathrm{H_2O}$ over a platinum surface. The nature of the chemicurrent has been debated in the literature; explanations both extrinsic and intrinsic to the reaction mechanism have been offered. This article suggests a picture behind the chemicurrent experiments, which is intrinsic to the mechanism of hydrogen oxidation in a high temperature regime. Surface reaction intermediates, $"\mathrm{O^-}"$, $"\mathrm{H^-}"$, $"\mathrm{OH^-}"$, are negatively charged while the product, $\mathrm{H_2O}$, and reactants, $\mathrm{H_2}$ and $\mathrm{O_2}$, are neutral. Hence, charge transfers between the metal and reacting species are inevitable. After electrons are transferred from the metal to the interface in dissociative oxygen and hydrogen adsorption, translationally excited electrons in the metal arise in part as a result of decay of negatively charged transition states in reaction steps connecting surface species of different charges, $"\mathrm{O^-+H^-}" \rightleftarrows "\mathrm{2 e+OH^-}"$ and $"\mathrm{OH^-+H^-}"\rightleftarrows "\mathrm{2 e+H_2O}"$. These transition states are the lowest energy configurations possible for changing the charge of the negatively charged surface intermediates. In particular, the transition state for $"\mathrm{O^-+H^-}" \rightleftarrows \mathrm{"2 e+OH^-"}$ limits the reaction rate. These processes may contribute to the chemicurrent. This picture should also apply to other catalytic chemical reactions on metal surfaces that proceed through formation of charged surface intermediates and their consequent discharge into the metal.
Low-Noble-Metal-Loading Hybrid Catalytic System for Oxygen Reduction Utilizing Reduced-Graphene-Oxide-Supported-Platinum Aligned with Carbon-Nanotube-Supported Iridium
由还原的氧化石墨烯负载的铂和多壁碳纳米管负载的铱(两种贵金属分别以15和< 5 μ g cm-2的水平的低负载量使用)组成的混合系统已被认为是用于在酸性介质(0.5 mol dm-3 H2SO 4)中还原氧的催化材料。用旋转环-盘电极伏安法测试了该催化剂对氧还原和过氧化氢中间体形成的电催化活性。所提出的催化系统的效率也通过在80 °C下用气体扩散电极半电池进行电流动力学测量来解决。碳纳米管的作用是通过降低溶剂蒸发过程中还原氧化石墨烯重新堆积的程度来改善电催化界面处的电荷分布,并促进催化系统中氧气和电解质的传输。诊断电化学实验揭示,在含铱的系统中,不仅产生了更高的盘电流,而且产生了小得多的环电流(与还原的氧化石墨烯负载的铂及其与裸碳纳米管的复合物相比),清楚地表明形成了较少量的不期望的过氧化氢中间体。在低负载下使用的来自向Pt添加痕量铱(负载在碳纳米管上)的增强效应可能源于Ir诱导不期望的过氧化氢中间体分解的高能力。在混合体系中,Pt活性中心的活化(由于少量Ir的存在)和稀释(通过碳纳米管)之间存在竞争,因此特别注意调整它们的组成。
Effect of CO desorption and coadsorption with O on the phase diagram of a Ziff-Gulari-Barshad model for the catalytic oxidation of CO
本文用Ziff-Gulari-Barshad模型(ZGB-d)研究了CO + O -> CO_2反应中CO和O的共吸附效应。CO在已经被O占据的表面位置上的共吸附通过以概率p,0 <= p <= 1发生的Eley-Rideal型机制引入。我们发现,除了众所周知的消除反应状态和O中毒状态之间的二级相变的效果,共吸附步骤有很强的影响反应状态和CO中毒状态之间的过渡。这两种状态之间的共存曲线终止于解吸速率k的临界值k_c,这取决于p。我们的蒙特卡罗模拟和有限尺寸尺度分析表明,k_c随p值的增加而减小。对于p=1,似乎只有当k为零(或接近零)时,两种状态之间才会出现急剧的相变。
Mechanistic Insights into Complete Methane Oxidation on Single-Atom Pd Supported by SSZ-13 Zeolite: A First-Principles Study
Korea Institute of Materials Science (KIMS)(韩国材料科学研究所);Indo-Korea Science and Technology Center (IKST)(印韩科学与技术中心);Electronic Materials Research Center, Korea Institute of Science & Technology(韩国科学技术院电子材料研究中心)
CO Oxidation Catalysed by Pd-based Bimetallic Nanoalloys
基于密度泛函理论的全局几何优化已被用来证明催化团簇的几何结构对Pd基纳米合金上CO氧化反应的能垒的关键影响。我们发现,反应中间体之间的巨大几何变化可能导致非常高的能量势垒,从而对整个过程是禁止的。这对新催化剂的设计和所采用的理论方法都提出了挑战。在理论方面,仔细选择所有反应中间体的几何构型对于充分描述可能的反应路径是至关重要的。从催化剂设计的角度来看,可以通过调节团簇和掺杂剂金属之间的相互作用水平来控制团簇的几何构型,以及通过在单个纳米合金颗粒中混合不同的金属而在吸附物分子和催化剂簇之间进行。我们发现,Pd $_{5}$簇中的Pd原子与单个Ag原子的取代形成Pd $_{4}$ Ag $_{1}$导致簇的CO氧化反应的催化性能的潜在改善。另一方面,一个单一的金原子不提高催化剂的性能,这是由于集群的组成金属和吸附分子之间的较弱的杂化。这种灵活性的性质的x-nanoalloy集群说明微调的可能性,这可能是用于设计新的高效催化材料。
CO oxidation on Pd(100) at technologically relevant pressure conditions: A first-principles kinetic Monte Carlo study
近年来,氧化物的形成对过渡金属多相氧化催化活性的影响引起了热烈的讨论。在更贵的过渡金属(如Pd、Pt或Ag)上,常见的本体氧化物的低稳定性主要表明亚纳米薄氧化物膜(所谓的表面氧化物)作为潜在的候选物,其可以在代表技术氧化催化的气相条件下稳定。我们解决了这个问题的Pd(100)模型催化剂表面的第一性原理动力学蒙特卡罗(kMC)模拟,评估稳定的表征(sqrt{5} x sqrt{5})R27表面氧化物在稳态CO氧化。我们的研究结果表明,在环境压力条件下,表面氧化物是稳定的表面CO:O2分压比附近的催化最相关的化学计量进料(p(CO):p(O2)= 2:1)。精确的值敏感地取决于温度,使得局部压力和温度波动都可能在环境化学计量条件下的稳态操作期间引起氧化物相的连续形成和分解。
University of Illinois(伊利诺伊大学);Materials Research Laboratory, University of Illinois(伊利诺伊大学材料研究实验室);Beckman Institute for Advanced Science and Technology, University of Illinois(伊利诺伊大学贝克曼先进科学技术研究所)
Surface states in bulk single crystal of topological semimetal Co$_3$Sn$_2$S$_2$ towards water oxidation
拓扑相物质的能带反转带来了奇异的物理性质,如拓扑保护表面态的出现。它们强烈地影响所研究材料的表面电子结构,并且可以作为一个很好的平台来深入了解表面反应的催化机制。在这里,我们合成了拓扑半金属Co $_3$ Sn $_2$ S $_2$的高质量块体单晶。我们发现,在室温下,Co $_3$ Sn $_2$ S $_2$自然地拥有拓扑半金属的能带结构。这就保证了Co原子表面态的存在。Co $_3$ Sn $_2$ S $_2$大块单晶暴露出由Co原子构成的Kagome晶格,具有高的电导率。它们作为析氧过程(OER)的催化中心,由于部分填充的$e_g$轨道,使成键和电子转移更有效。该块体单晶显示出优异的OER催化性能,尽管表面积比Co基纳米结构催化剂小得多。我们的研究结果强调了裁剪拓扑非平凡的表面状态的高活性电催化剂的合理设计的重要性。
On the evolution of oxidative etching of few layer graphene (FLG) in FLG /TiO$_2$ nanocomposites. Interfacial dipole signature and chemical shift in C1s X-ray photoemission spectra
Effect of surface nanostructure on temperature programmed reaction spectroscopy: First-principles kinetic Monte Carlo simulations of CO oxidation at RuO2(110)
Magnetically collected platinum/nickel alloy nanoparticles -- insight into low noble metal content catalysts for hydrogen evolution reaction
析氢反应(HER)是电化学分解水的关键过程。为了降低该过程的成本和环境影响,开发具有低含量或不含贵金属的电催化剂是非常有动机的。在这里,我们报告了一种新颖的和巧妙的合成混合PtxNi1-x电催化剂的形式的纳米粒子的项链结构命名为nanotrusses,具有非常低的贵金属含量。纳米桁架结构具有重要的特征,例如良好的导电性、高表面积、强的互连和基底粘附性,这使得具有优异的HER活性。具体而言,表现最好的Pt0.05Ni0.95样品在0.5 M H2SO4中的塔菲尔斜率为30 mV dec-1,在10 mA cm-2的电流密度下的过电位为20 mV,具有高稳定性。令人印象深刻的催化性能在理论研究中得到了进一步的合理化,该理论研究深入了解了这种小铂含量如何使氢的吸附能接近最佳的机制。
An Atomic-Scale View of CO and H2 Oxidation on a Pt-Fe3O4 Model Catalyst
金属-载体相互作用经常被用来解释分散在可还原的金属氧化物载体上的金属纳米颗粒的增强的催化活性,但原子尺度的机制很少有人知道。在这里,我们使用扫描隧道显微镜研究Pt 1 -6/Fe 3 O 4模型催化剂暴露于CO,H2,O2,及其混合物,在550 K。CO在簇周边提取晶格氧以形成CO2,在金属氧化物表面产生大孔。H2和O2在金属簇上解离并溢出到载体上。前者产生表面羟基,其与载体反应以解吸水,而原子氧与本体中的Fe反应以产生新的Fe 3 O 4(001)岛。铂的存在是至关重要的,因为它催化已经发生在裸露的氧化铁表面上的反应,但在更高的温度下。
Using a dual plasma process to produce cobalt--polypyrrole catalysts for the oxygen reduction reaction in fuel cells -- part I: characterisation of the catalytic activity and surface structure
介绍了一种新的双等离子体涂层工艺,用于制备燃料电池中氧还原反应的无铂催化剂。用各种方法分析由此产生的催化剂。通过循环伏安法、旋转环电极和旋转环盘电极进行电化学表征。由此获得的不同的催化剂的表面孔隙率的特征在于与氮气吸附技术和扫描电子显微镜用于确定膜的生长机制。它表明,催化活性化合物可以用这种双等离子体工艺生产。此外,催化活性可以通过改变等离子体工艺参数而显著变化。计算了生成的H $_2$ O $_2$的量,并表明2电子机理是主要的。等离子体涂覆机制不会显著改变所用碳载体的表面BET面积和孔径分布。此外,所产生的薄膜的扫描电子显微镜照片,并示出的柱状生长机制的偏好。通过使用不同的碳作为载体,它表明,有很强的依赖性的催化活性,这可能是有关的碳的化学性质。
Sonochemically Boosted Hydrogen Evolution Activity of Janus TMD Monolayers
Tata Institute of Fundamental Research(塔塔基础研究所);Friedrich Schiller University Jena(耶拿弗里德里希·席勒大学);Helmholtz-Zentrum Dresden-Rossendorf(德累斯顿-罗斯多夫亥姆霍兹中心);Center for Energy and Environmental Chemistry(能源与环境化学中心)
Transient Surface Oxides Form on Pt(111) - But Vanish During Ammonia Oxidation
Synchrotron SOLEIL(SOLEIL同步辐射中心);Université Grenoble Alpes, CEA Grenoble, IRIG, MEM, NRX(格勒诺布尔阿尔卑斯大学,CEA格勒诺布尔,IRIG,MEM,NRX);Laboratoire Matériaux et Phénomènes Quantiques, Université Paris Cité, CNRS(材料与量子现象实验室,巴黎西岱大学,法国国家科学研究中心);European Synchrotron Research Facility(欧洲同步辐射装置)
Exploring the role of electronic structure on photo-catalytic behavior of carbon-nitride polymorphs
一个完全自洽的密度泛函理论(DFT)与改进的功能是用来提供一个全面的帐户的结构,电子和光学性质的C $_{3}$ N $_{4}$多晶型物。使用我们最近开发的van Leeuwen-Baerends(vLB)修正局域密度近似(LDA),我们在全势N $^{th}$阶松饼丁轨道(FP-NMTO)方法中实现了LDA+vLB,并表明与半局域泛函(LDA/GGA)相比,它改善了结构性质和带隙。我们证明,LDA+vLB预测的能带结构和功函数的良好研究的2D-石墨烯和体硅在非常好的协议与实验,和更精确的混合功能(HSE)的计算中实现的量子浓缩咖啡(QE)包。使用FP-NMTO-LDA+vLB计算的C $_{3}$ N $_{4}$多晶型物的结构和电子结构(带隙)特性与更复杂的混合泛函计算进行了比较。我们还使用QE-HSE方法通过功函数、能带(价和传导)位置相对于水还原和氧化电位对C $_{3}$ N $_{4}$多晶型物的光催化行为进行了详细的研究。我们的研究结果表明,$γ$ -C $_{3}$ N $_{4}$是所有C $_{3}$ N $_{4}$ ~多晶型体中最好的候选者,但它在“零”压力下是动态不稳定的。我们发现$γ$ -C $_{3}$ N $_{4}$可以在流体静压下稳定,这改善了其相对于水还原和氧化电位的光催化行为。