坩埚下降法生长掺碲化铅晶体中Eu杂质的偏析与浓度的关系
Segregation of the Eu impurity as function of its concentration in the melt for growing of the lead telluride doped crystals by the Bridgman method
摘要:
本文用X射线荧光元素分析、次级中性质谱(SNMS)和磁性测量研究了不同初始杂质N浓度(约1 × 10 ~(19)cm ~(-3)及以下)的坩埚下降法生长的PbTe单晶中稀土杂质Eu的行为。建立了沿掺杂锭和跨掺杂锭的杂质分布。结果表明,只有当掺杂杂质在熔体中的初始浓度足够高(约为1 × 10 ~(-3)+20 cm ~(-3))时,掺杂杂质才能进入掺杂晶体的本体中。如果该浓度较低,约为1 × 10+19 cm-3或更低,则掺杂Eu杂质被挤出到掺杂锭的表面上。掺杂表面层的厚度估计为几微米或更大。当N=1 × 10+20 cm-3时,Eu杂质沿晶锭轴向的纵向分布以及当N=1 × 10+19 cm-3时,杂质全部被挤出的表面层中的横向分布都是强非单调的。分析了熔体法生长PbTe:Eu晶体过程中Eu掺杂杂质异常行为的可能原因。
英文摘要:
Behaviour of a rare earth impurity of Eu in the PbTe single crystals grown by the Bridgman method from the melt with different initial concentrations of impurity N about 1*10+19 cm-3 and less is investigated with X-ray fluorescent element analysis, Secondary Neutral Mass Spectroscopy (SNMS), and magnetic measurements. The impurity distributions along and across the doped ingots are established. It is revealed that doping impurity enters into the bulk of doped crystals only if its initial concentration in the melt is high enough, approximately 1*10+20 cm-3. If this concentration is lower, about 1*10+19 cm-3 and less, the doping Eu impurity is pushed out onto the surface of doped ingot. The thickness of the doped surface layer is estimated to be in the order of several microns or somewhat more. The longitudinal distributions of Eu impurity along the axis of doped ingot for N=1*10+20 cm-3, as well as the transverse one in the surface layer where entire doping impurity is pushed out for N=1*10+19 cm-3, are strongly non-monotonic. Possible reasons for this unusual behaviour of Eu doping impurity during the growth of PbTe:Eu crystals from the melt are analyzed.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。