纤维上纳米颗粒悬浮液薄膜中的环形裂纹

Annular cracks in thin films of nanoparticle suspensions drying on a fiber

François Boulogne, Ludovic Pauchard, Frédérique Giorgiutti-Dauphiné

摘要:

我们报告的实验研究过程中形成的裂纹图案的胶体悬浮液干燥。提供一维无边界基底的水平纤维被微米厚度的膜涂覆。几何形状强加了一个显着的环形裂纹图案,并允许精确测量的裂纹间距在一个很短的范围内的膜厚度(2和10 $μ$ m之间),其随膜高度线性变化。我们比较了我们的实验数据与Kitsunezaki提出的模型,该模型表明裂纹间距随膜厚度的变化取决于开裂时的临界应力和在基板上滑动的临界应力之间的比率。通过悬臂梁技术测量胶体凝胶在疏水表面上的摩擦力,我们可以简单地通过测量图案的裂纹间距来推断这些胶体凝胶的临界裂纹应力。

英文摘要:

We report an experimental study of the crack pattern formed during the drying of a colloidal suspension. A horizontal fiber, which provides a one dimensional, boundary-free substrate, is coated by a film of micronic thickness. The geometry imposes a remarkable annular crack pattern and allowing precise measurements of the crack spacing over a short range of film thickness (between 2 and 10 $μ$m) which varies linearly with the film height. We compare our experimental data with a model proposed by Kitsunezaki which suggests that the variation of the crack spacing with the film thickness depends on the ratio between a critical stress at cracking and a critical stress for slipping on the substrate. By measuring the friction force of the colloidal gels on a hydrophobic surface through a cantilever technique, we can deduce the critical crack stress for these colloidal gels simply by measuring the crack spacing of the pattern.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑