Ni(111)表面二维硅化镍的形成和稳定性俄歇、LEED、STM和高分辨光电能谱研究
Formation and stability of a two-dimensional nickel silicide on Ni (111) an Auger, LEED, STM, and high-resolution photoemission Study
摘要:
利用低能电子衍射(LEED)、俄歇电子能谱(AES)、扫描隧道显微镜(STM)和高分辨光电子能谱(HR-PES)等技术,研究了室温下沉积在Ni(111)衬底上的单层硅的退火效应。通过AES在300°C和400°C下记录的Si表面浓度的变化显示,在开始时,Si快速降低,随后减慢至相当于约1/3硅单层的平台。退火后在室温下记录的STM图像和LEED图案揭示了有序六方超结构(rot 3xrot 3)R30°型的形成。从这些观察和从HR-PES数据的定量分析,记录退火前后,我们提出,(rot 3 × rot 3)R30°超结构对应于一个二维(2D)Ni 2Si表面硅化物。
英文摘要:
Using low energy electron diffraction (LEED), Auger electron spectroscopy (AES), scanning tunnelling microscopy (STM) and high resolution photo-electron spectroscopy (HR-PES) techniques we have studied the annealing effect of one silicon monolayer deposited at room temperature onto a Ni (111) substrate. The variations of the Si surface concentration, recorded by AES at 300°C and 400°C, show at the beginning a rapid Si decreasing followed by a slowing down up to a plateau equivalent to about 1/3 silicon monolayer. STM images and LEED patterns, both recorded at room temperature just after annealing, reveal the formation of an ordered hexagonal superstructure(rot3xrot3)R30°-type. From these observations and from a quantitative analysis of HR-PES data, recorded before and after annealing, we propose that the (rot3 x rot3)R30°superstructure corresponds to a two dimensional (2D) Ni2Si surface silicide.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。