摘要:

在这项研究中,镍薄膜沉积的远程等离子体原子层沉积(RPALD)的p型硅衬底和硅化镍的形成,使用快速热退火的特性进行了测定。使用双(1,4-二异丙基-1,3-二氮杂丁二烯基)镍Ni(iPr-DAD)2作为Ni前体,并使用氨等离子体作为反应物。这是首次尝试使用Ni(iPr-DAD)2作为ALD工艺的前体来沉积Ni薄膜。RPALD Ni膜在250 °C下以约2.2欧姆/循环的生长速率沉积,并且显示出33 μΩcm的显著低电阻率,总杂质浓度约为10原子%。该薄膜的杂质碳和氮以C-C和C-N的形式以键合状态存在。通过对实验条件(温度和压力)的比较,考察了杂质的去除趋势.在每个ALD循环期间通过热脱附去除氮杂质,并且通过优化与NH3等离子体的平均自由程直接相关的工艺压力来减少碳杂质。在Ni沉积之后,在真空环境中通过RTA形成硅化镍1分钟。在500至900 °C的退火温度下比较来自ALD Ni和PVD Ni的硅化镍层。由于沉积态Ni薄膜中少量的碳和氮的贡献,由ALD Ni制备的NiSi具有更好的热稳定性。使用ALD Ni有效地抑制了硅化物层的退化。

英文摘要:

In this study, the characteristics of nickel thin film deposited by remote plasma atomic layer deposition (RPALD) on p-type Si substrate and formation of nickel silicide using rapid thermal annealing were determined. Bis(1,4-di-isopropyl-1,3-diazabutadienyl)nickel, Ni(iPr-DAD)2, was used as a Ni precursor and ammonia plasma was used as a reactant. This was the first attempt to deposit Ni thin film using Ni(iPr-DAD)2 as a precursor for the ALD process. The RPALD Ni film was deposited with a growth rate of around 2.2Å/cycle at 250 °C and showed significant low resistivity of 33 μΩcm with a total impurity concentration of around 10 at. %.The impurities of the thin film, carbon and nitrogen, were existent by the forms of C-C and C-N in a bonding state. The impurities removal tendency was investigated by comparing of experimental conditions, namely process temperature and pressure. Nitrogen impurity was removed by thermal desorption during each ALD cycle and carbon impurity was reduced by the optimizing of the process pressure which is directly related with a mean free path of NH3 plasma. After Ni deposition, nickel silicide was formed by RTA in a vacuum ambient for 1 minute. A nickel silicide layer from ALD Ni and PVD Ni was compared at the annealing temperature from 500 to 900 °C. NiSi from ALD Ni showed better thermal stability due to the contribution of small amounts of carbon and nitrogen in the asdeposited Ni thin film. Degradation of the silicide layer was effectively suppressed with a use of ALD Ni.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑