arXivDaily arXiv每日学术速递 周一至周五更新
arXiv 1301.5341cond-mat.supr-con
收藏

银的内部气体和蠕变在控制银护套Bi2Sr2CaCu2Ox丝临界电流密度中的作用

Role of internal gases and creep of Ag in controlling the critical current density of Ag-sheathed Bi2Sr2CaCu2Ox wires

T. Shen, A. Ghosh, L. Cooley, J. Jiang

摘要:

在20 T和4.2 K下,当试样长度为几厘米时,Ag包套多芯Bi_2Sr_2CaCu_2 O_x(Bi-2212)圆丝可获得大于500 A/mm ~ 2的高工程临界电流密度JE。然而,在几米长的Bi-2212导线以及缠绕成线圈的较长段中,JE(20 T)很少超过200 A/mm 2。此外,长长度的线通常在熔融加工后表现出Bi-2212泄漏的迹象,这在短的开口端样品中很少发现。我们使用质谱法研究了最先进的管中粉末(PIT)Bi-2212线的JE的长度依赖性和在熔融加工期间由它们释放的气体,证实JE随长度的降解是由于在升高的温度下由高内部气体压力产生的线溶胀[1,2]。我们进一步模拟了Bi-2212线材中的气体传输,并检查了在熔融加工前的拉制PIT线材和接受脱气处理或冷致密化处理的线材的熔融加工的关键阶段的线材膨胀。这些研究表明,在长的长度线的内部气体压力驱动蠕变的Ag护套在热处理过程中,导致线膨胀,降低密度的Bi-2212细丝,并因此降低线JE;蠕变断裂的银护套自然导致泄漏的Bi-2212液体。我们的工作表明,适当控制这种蠕变是防止Bi-2212泄漏和在长Bi-2212导体和线圈中实现高JE的关键。

英文摘要:

High engineering critical current density JE of >500 A/mm2 at 20 T and 4.2 K can be regularly achieved in Ag-sheathed multifilamentary Bi2Sr2CaCu2Ox (Bi-2212) round wire when the sample length is several centimeters. However, JE(20 T) in Bi-2212 wires of several meters length, as well as longer pieces wound in coils, rarely exceeds 200 A/mm2. Moreover, long-length wires often exhibit signs of Bi-2212 leakage after melt processing that are rarely found in short, open-end samples. We studied the length dependence of JE of state-of-the-art powder-in-tube (PIT) Bi-2212 wires and gases released by them during melt processing using mass spectroscopy, confirming that JE degradation with length is due to wire swelling produced by high internal gas pressures at elevated temperatures [1,2]. We further modeled the gas transport in Bi-2212 wires and examined the wire expansion at critical stages of the melt processing of as-drawn PIT wires and the wires that received a degassing treatment or a cold-densification treatment before melt processing. These investigations showed that internal gas pressure in long-length wires drives creep of the Ag sheath during the heat treatment, causing wire to expand, lowering the density of Bi-2212 filaments, and therefore degrading the wire JE; the creep rupture of silver sheath naturally leads to the leakage of Bi-2212 liquid. Our work shows that proper control of such creep is the key to preventing Bi-2212 leakage and achieving high JE in long-length Bi-2212 conductors and coils.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑