arXivDaily arXiv每日学术速递 周一至周五更新
感恩节,周五至周末无更新,大家顺遂。周一再来吧
arXiv 1301.4018cond-mat.mtrl-scicond-mat.str-el
收藏

衬底对双临界$Sm_{0.53} Sr_{0.47} Mn O_3$薄膜磁相共存的影响

Impact of substrate on magnetic phase coexistence in bicritical $Sm_{0.53} Sr_{0.47} Mn O_3$ thin films

M. K. Srivastava, M. P. Singh, P. K. Siwach, A. Kaur, F. S. Razavi, H. K. Singh

摘要:

采用直流磁控溅射法在LaAlO 3(LAO/(001))和SrTiO 3(STO/(001))单晶衬底上制备了Sm 0. 53 Sr 0. 47 MnO 3薄膜。θ-2 θ和ω-2 θ扫描表明,这些薄膜具有非常好的结晶度,LAO和STO上的薄膜分别处于压缩和拉伸应变下。LAO和STO衬底上的薄膜分别在TC \sim 126 K(TIM \sim 128 K)和120 K(TIM \sim 117 K)处显示铁磁(绝缘体-金属)转变。在T<TC的磁性状态类似于团簇玻璃,其由铁磁基质中存在的电荷有序反铁磁团簇形成。在TIM电阻率的巨大下降和相关的滞后相对于冷却和加热循环揭示了双临界和一级性质的相变,这也证实了Banerjee准则。薄膜的功能特性的差异和相似之处解释在衬底改性的磁相共存。

英文摘要:

Sm0.53Sr0.47MnO3 thin films were deposited on single crystal LaAlO3 (LAO/(001)) and SrTiO3 (STO/(001)) substrates by DC magnetron sputtering. The theta-2theta and omega-2theta scans show that these films have very good crystallinity and the films on LAO and STO are under compressive and tensile strain, respectively. The films on LAO and STO substrates show ferromagnetic (insulator-metal) transition at TC \sim 126 K (at TIM \sim 128 K) and 120 K (TIM \sim 117K), respectively. The magnetic state at T<TC is akin to cluster glass, which is formed by the presence of charge ordered-antiferromagnetic clusters in the ferromagnetic matrix. Huge drop in the resistivity at TIM and the associated hysteresis with respect to cooling and warming cycles reveal the bicritical and the first order nature of phase transition, which is also confirmed by the Banerjee criterion. The differences and similarities in the functional properties of films are explained in terms of substrate modified magnetic phase coexistence.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑