arXivDaily arXiv每日学术速递 周一至周五更新
arXiv 1207.4544cond-mat.mtrl-sci
收藏

棒状β'析出相的尺寸和分布对Mg-Zn合金强度和塑性的影响

The effect of size and distribution of rod-shaped β' precipitates on the strength and ductility of a Mg-Zn alloy

Julian M. Rosalie, Hidetoshi Somekawa, Alok Singh, Toshiji Mukai

摘要:

本文定量研究了Mg-Zn合金中β'相的尺寸和分布对强度和塑性的影响。尽管沉淀强化对于镁合金的实际应用至关重要,但本研究首次系统地研究了控制变形对沉淀物尺寸分布以及由此产生的镁合金强度和延展性的影响。采用预时效变形,通过非均匀形核获得不同分布的棒状β'析出相。挤压合金以获得织构,从而避免形成孪晶,从而确保位错是主要的成核位点。预时效应变细化了沉淀相的长度和直径,平均长度从440 nm减小到60 nm,直径从14 nm减小到9 nm。从显微照片中测量颗粒间距,并表明沉淀物分布中存在一些不均匀性。合金的屈服应力从273 MPa提高到309 MPa。屈服应力线性增加的倒数颗粒间的间距的函数,但在一个较低的速率比Orowan强化预测。预时效变形也导致延展性的显著损失(从17%至6%的伸长率)。在失败和均匀伸长率的真实应变表现出与颗粒间距的线性关系,在协议的非变形障碍物周围的位错的积累模型。与未变形的材料相比,经受3%预时效变形的样品显示出显著增加的时效响应;然而,额外的变形(至5%应变)仅导致沉淀物分布和机械性能的适度变化。

英文摘要:

We report on a quantitative investigation into the effect of size and distribution of rod-shaped β' precipitates on strength and ductility of a Mg-Zn alloy. Despite precipitation strengthening being crucial for the practical application of magnesium alloys this study represents the first systematic examination of the effect of controlled deformation on the precipitate size distribution and the resulting strength and ductility of a magnesium alloy. Pre-ageing deformation was used to obtain various distributions of rod-shaped β' precipitates through heterogeneous nucleation. Alloys were extruded to obtain a texture so as to avoid formation of twins and thus to ensure that dislocations were the primary nucleation site. Pre-ageing strain refined precipitate length and diameter, with average length reduced from 440 nm to 60 nm and diameter from 14 nm to 9 nm. Interparticle spacings were measured from micrographs and indicated some inhomogeneity in the precipitate distribution. The yield stress of the alloy increased from 273 MPa to 309 MPa. The yield stress increased linearly as a function of reciprocal interparticle spacing, but at a lower rate than predicted for Orowan strengthening. Pre-ageing deformation also resulted in a significant loss of ductility (from 17% to 6% elongation). Both true strain at failure and uniform elongation showed a linear relationship with particle spacing, in agreement with models for the accumulation of dislocations around non-deforming obstacles. Samples subjected to 3% pre-ageing deformation showed a substantially increased ageing response compared to non-deformed material; however, additional deformation (to 5% strain) resulted in only modest changes in precipitate distribution and mechanical properties.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑