氧化铁纳米粒子在250°C ~ 900°C温度处理过程中结构性质的演变:X射线衍射和Fe K壳层前边缘X射线吸收研究

Evolution of structural properties of iron oxide nano particles during temperature treatment from 250°C - 900°C: X-ray diffraction and Fe K-shell pre-edge X-ray absorption study

Debajeet K. Bora, Artur Braun, Selma Erat, Olga Safonova, Thomas Graule, Edwin C. Constable

摘要:

通过湿软化学方法在空气中热处理温度为250°C至900°C合成了具有名义Fe 2 O3化学计量比的氧化铁纳米颗粒。通过X射线衍射和Fe K壳层X射线吸收研究了纳米粒子的结构性质随热处理温度的变化。X射线衍射图表明,在较低的退火温度下,纳米颗粒包括磁赤铁矿和赤铁矿相。随着温度的升高,剩余的磁赤铁矿相完全转变为赤铁矿。主要布拉格反射的轮廓分析表明,随着温度的升高,平均晶粒尺寸从50 nm增加到150 nm。随着热处理温度的升高,平均一次粒径从105 nm减小到90 nm。X射线衍射结果通过Fe K-边缘X射线吸收光谱的边缘前结构的系统变化,特别是通过两个前沿边缘前共振的t2 g/eg峰高比的逐渐减小而被证实,证实Fe从Fe 2+向Fe 3+氧化。在高达900°C的温度下处理的样品上的透射电子显微镜(TEM)显示具有棱柱形态的颗粒以及堆垛层错样缺陷的形成。对350°C以上热处理的样品进行高分辨率TEM和选区电子衍射(SAED)分析,结果表明纳米颗粒具有与赤铁矿(110)晶面相对应的良好的晶格条纹。

英文摘要:

Iron oxide nano particles with nominal Fe2O3 stoichiometry were synthesized by a wet, soft chemical method with the heat treatment temperatures from 250°C to 900°C in air. The variation in the structural properties of the nano particles with the heat treatment temperature was studied by X-ray diffraction and Fe K shell X-ray absorption study. X-ray diffractograms show that at lower annealing temperatures nano particle comprises both maghemite and hematite phases. With increasing temperature, the remainder of the maghemite phase transformed completely to hematite. Profile analysis of the leading Bragg reflections reveals that the average crystallite size increases from 50 nm to 150 nm with increasing temperature. The mean primary particle size decreased from 105 nm to 90 nm with increasing heat treatment temperature. The X-ray diffraction results are paralleled by systematic changes in the pre-edge structure of the Fe K-edge X-ray absorption spectra, in particular by a gradual decrease of the t2g/eg peak height ratio of the two leading pre-edge resonances, confirming oxidation of the Fe from Fe2+ towards Fe3+. Transmission electron microscopy (TEM) on the samples treated at temperatures as high as 900°C showed particles with prismatic morphology along with the formation of stacking fault like defects. High resolution TEM with selected area electron diffraction (SAED) of samples heat treated above 350°C showed that the nano particles have well developed lattice fringes corresponding to that of (110) plane of hematite.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑