The AC susceptibility at zero DC magnetic field of a polycrystalline sample of LaFeAsO_{0.94}F_{0.06} (T_c = 24 K) has been investigated as a function of the temperature, the amplitude of the AC magnetic field (in the range Hac = 0.003 - 4 Oe) and the frequency (in the range f = 10 kHz - 100 kHz). The temperature dependence of the AC susceptibility exhibits the typical two-step transition arising from the combined response of superconduncting grains and intergranular weak-coupled medium. The intergranular part of the susceptibility strongly depends on both the amplitude and the frequency of the AC driving field, from few Kelvin below T_c down to T = 4.2 K. Our results show that, in the investigated sample, the intergrain critical current is not determined by pinning of Josephson vortices but by Josephson critical current across neighboring grains.
Structural and electronic properties of LaFeAsO$_{0.85}$F$_{0.15}$ superconductor modified under neutron irradiation
用X射线衍射和$^{75}$ As NMR研究了中子辐照引起的原子无序对轻过掺杂LaFeAsO $_{0.85}$ F $_{0.15}$($T_c=21K$)晶体结构和$E_F$附近电子态的影响.在$T=50^{\circ}C$上用“中等”注量的$Φ=(0;0.5;1.6)\cdot10^{19}cm^{-2}$中子辐照多晶样品导致超导性的抑制。结果表明,中子辐照产生的四方晶系晶格的各向异性膨胀几乎是由于Fe-As距离的增加。的FeAs层的2D字符的部分损失是伴随着抑制的自旋磁化率的温度依赖性的间隙状功能。在最无序的状态下,$^{75}$ As的自旋-晶格弛豫速率遵循柯林加定律$^{75}T_1^{-1} \sim T$,热行为对于传导电子的各向同性运动是典型的。
A unified phase diagram of F-doped LaFeAsO by means of NMR and NQR parameters
我们目前$^{75}$作为核磁共振和四极共振结果(NMR,NQR)的一组新的LaFeAsO $_{1-x}$ F $_x$多晶样品。改进的合成条件导致更均匀的样品,更好地控制氟含量。结构$\equiv$的磁,超导转变温度已被确定的NMR自旋晶格弛豫率和交流磁化率测量。如此确定的相图偏离公布的一个,特别是低F掺杂浓度。然而,如果从NQR谱确定掺杂水平,则两个相图可以被调和。磁性和超导性的本体共存和纳米级分离成低掺杂样和高掺杂样区域的情况下,已被证实。在磁性和超导性的边界处对欠掺杂样品的附加频率依赖的强度、自旋-自旋和自旋-晶格弛豫率测量表明,正交性和磁性起源于低掺杂区,超导性首先在高掺杂区发展。
Hysteresis and stepwise structure in MR curves of granular superconducting ruthenocuprates RuSr$_2$(Gd$_{1.5}$Ce$_{0.5})$Cu$_2$O$_{10-δ}$}
本文研究了六元铜酸盐RuSr $_2$(Gd $_{1.5}$ Ce $_{0.5})$ Cu $_2$ O $_{10-δ}$)多晶样品的颗粒超导电性效应。主要的注意力一直致力于表现出这些影响的电流和磁场的依赖性的电阻过渡到超导状态。发现不同温度下微分电阻随电流的变化关系在两个确定的电流值处严格相交,表现出交叉点效应。这一现象已被解释考虑到晶粒间介质的非均匀状态,可以被认为是一个两个组件系统。特别关注了该非均匀系统混合状态下的磁电阻(MR)滞后以及施加电流和温度对这种现象的影响。两种类型的滞后(顺时针和逆时针)已被发现与过渡从顺时针到逆时针滞后随着温度的升高。在低场范围内,观察到了MR迟滞曲线的阶梯结构。考虑到所研究的颗粒超导体的非均匀状态,讨论了磁滞行为随温度升高而变化以及MR曲线中出现阶梯结构的可能原因。
Single-crystal growth of iron-based superconductor La$_{0.34}$Na$_{0.66}$Fe$_2$As$_2$
本文报道了La $_{0.34}$ Na $_{0.66}$ Fe $_2$ As $_2$铁基超导体的单晶生长,其尺寸为几毫米。这些样品是在试图用NaAs和NaF助熔剂生长LaFeAsO $_{1-y}$ F $_y$($y \geq$ 0.8)单晶时意外获得的。样品在106 K下同时表现出反铁磁和结构转变。超导转变温度约为27 K,超导各向异性约为1.9。这些值和霍尔系数的温度依赖性表明La $_{0.34}$ Na $_{0.66}$ Fe $_2$ As $_2$属于空穴掺杂的铁磷属元素化物的“122”族,掺杂水平略低于最佳掺杂。与以前报道的多晶样品相比,我们的结果表明,该系统的$T_c$可以进一步增加,或者超导圆顶可能在该系统中没有很好地形成。无论哪种情况,La $_{0.5-x}$ Na $_{0.5+x}$ Fe $_2$ As $_2$体系都为研究铁基超导体的反铁磁和超导性质提供了一个新的平台。