金属薄膜如何对基材进行去湿--识别动力学路径和能量驱动力

How metal films de-wet substrates - identifying the kinetic pathways and energetic driving forces

Kevin F. McCarty, John C. Hamilton, Yu Sato, Angela Saa, Roland Stumpf, Juan de la Figuera, Konrad Thurmer, Frank Jones, Andreas K. Schmid, A. Alec Talin, Norman C. Bartelt

摘要:

我们研究了W(110)衬底上均匀厚度的单晶铬膜在退火过程中如何转化为三维(3D)Cr岛阵列。我们使用低能电子显微镜(LEEM)直接观察的动力学途径,产生暴露的润湿层的沟槽。相邻的膜台阶相对于衬底上的原子台阶的阶梯同时向上和向下移动。这种步进运动使步进前进的胶片区域变厚。在薄膜台阶缩回的地方,薄膜变薄,最终暴露出稳定的润湿层。由于我们的分析表明,厚铬膜的晶格常数接近散装铬,我们建议,表面和界面应力提供了一个可能的驱动力所观察到的形态不稳定。原子模拟和分析弹性模型表明,表面和界面应力可以导致膜能量对厚度的依赖性,从而导致同时变薄和增厚的不稳定性。我们观察到,去湿也开始在两个其他系统,Ag/W(110)和Ag/Ru(0001)的衬底台阶束。我们还描述了如何将Cr膜转换成单向条纹的图案,因为暴露润湿层的沟槽沿着W[001]方向延长。最后,我们观察如何直接在薄膜生长过程中在高温下形成3D Cr岛。当Cr膜台阶沿着衬底台阶的阶梯向下前进时,Cr台面(楔形)形成,这是衬底台阶在3D岛形成中起关键作用的另一个示例。

英文摘要:

We study how single-crystal chromium films of uniform thickness on W(110) substrates are converted to arrays of three-dimensional (3D) Cr islands during annealing. We use low-energy electron microscopy (LEEM) to directly observe a kinetic pathway that produces trenches that expose the wetting layer. Adjacent film steps move simultaneously uphill and downhill relative to the staircase of atomic steps on the substrate. This step motion thickens the film regions where steps advance. Where film steps retract, the film thins, eventually exposing the stable wetting layer. Since our analysis shows that thick Cr films have a lattice constant close to bulk Cr, we propose that surface and interface stress provide a possible driving force for the observed morphological instability. Atomistic simulations and analytic elastic models show that surface and interface stress can cause a dependence of film energy on thickness that leads to an instability to simultaneous thinning and thickening. We observe that de-wetting is also initiated at bunches of substrate steps in two other systems, Ag/W(110) and Ag/Ru(0001). We additionally describe how Cr films are converted into patterns of unidirectional stripes as the trenches that expose the wetting layer lengthen along the W[001] direction. Finally, we observe how 3D Cr islands form directly during film growth at elevated temperature. The Cr mesas (wedges) form as Cr film steps advance down the staircase of substrate steps, another example of the critical role that substrate steps play in 3D island formation.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑