硅晶圆上的钒超导微波谐振器
Vanadium superconducting microwave resonators on silicon wafers
AI总结:
研究钒薄膜的结构性质与微波损耗的关联,发现表面损耗主要由非二能级系统损耗主导,可通过钽覆盖层缓解,而铌缓冲层虽提高晶格取向均匀性却增加非二能级系统损耗。
摘要:
理解超导薄膜中材料性质与微波损耗之间的关联是开发用于量子电路的低损耗材料的关键课题。我们关注钒(V)作为超导量子器件的新型材料,并讨论V薄膜的损耗与其结构性质的关系。采用溅射方法,在(001)取向的Si晶圆上生长四种V薄膜结构,分别使用Nb和Ta作为缓冲层和覆盖层材料:Nb/V/Ta、Nb/V、V/Ta和V。X射线衍射和原子力显微镜显示,在Nb缓冲层上生长的V薄膜比直接在Si晶圆上生长的V薄膜具有更高的晶格取向均匀性和更小的晶粒尺寸。从四种V薄膜结构制备共面波导谐振器,通过微波测量获得内部品质因子($Q_{\rm int}$)对平均光子数($\langle n_{\rm ph} \rangle$)的依赖关系。通过分析得到的$Q_{\rm int}$ vs $\langle n_{\rm ph} \rangle$,发现V表面的损耗主要由与$\langle n_{\rm ph} \rangle$无关的非二能级系统(非TLS)损耗主导,这可以通过引入Ta覆盖层来缓解。此外,在$\langle n_{\rm ph} \rangle$范围从10$^{0}$到10$^{6}$内,Nb缓冲层上的V薄膜表现出比直接在Si晶圆上生长的V薄膜更低的$Q_{\rm int}$和更高的非TLS损耗,尽管前者具有更高的晶格取向均匀性。这些趋势的起源可能与V氧化物有关,能量色散X射线光谱和X射线光电子能谱表明在V谐振器的表面和体区域晶界处存在V氧化物,和/或与V氢化物有关。
英文摘要:
Understanding the correlation between material properties and microwave losses in superconducting films is a crucial subject for developing low-loss materials for quantum circuits. We focus on vanadium (V) as a novel material for superconducting quantum devices and discuss loss in V films in relation to their structural properties. Using a sputtering method, we grow four V-film structures on (001)-oriented Si wafers, employing Nb and Ta as the buffer and capping layer materials, respectively: Nb/V/Ta, Nb/V, V/Ta, and V. X-ray diffraction and atomic force microscopy reveal that the V films grown on the Nb buffer layers have higher uniformity of lattice orientation and smaller grain size than that directly grown on the Si wafer. Coplanar waveguide resonators are fabricated from the four V-film structures, and averaged photon number ($\langle n_{\rm ph} \rangle$) dependences of internal quality factor ($Q_{\rm int}$) are obtained by performing microwave measurements. By analyzing the obtained $Q_{\rm int}$ vs $\langle n_{\rm ph} \rangle$, it is found that loss at the V surface is dominated by $\langle n_{\rm ph} \rangle$-independent non-two-level-system (non-TLS) losses, which can be mitigated by introducing the Ta capping layer. Furthermore, the V films on the Nb buffer layers exhibit lower $Q_{\rm int}$ in the $\langle n_{\rm ph} \rangle$ range from 10$^{0}$ to 10$^{6}$ and higher non-TLS loss than that directly grown on Si wafers, even though the former has higher lattice-orientation uniformity than the latter. Origins of these trends might be relevant to V oxides, of which presence at surfaces and grain boundaries in bulk regions in the V resonators is suggested by energy dispersive X-ray spectroscopy and X-ray photoelectron spectroscopy, and/or V hydrides.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。