State Key Laboratory of Solid Lubrication, Lanzhou Institute of Chemical Physics, Chinese Academy of Sciences(中国科学院兰州化学物理研究所固体润滑国家重点实验室);Department of Engineering Mechanics, School of Civil Engineering, Wuhan University(武汉大学土木工程学院工程力学系);State Key Laboratory of Water Resources Engineering and Management, Wuhan University(武汉大学水资源与水电工程科学国家重点实验室);Center of Materials Science and Optoelectronics Engineering, University of Chinese Academy of Sciences(中国科学院大学材料科学与光电技术研究中心)

Wan Wang, Zijun Ding, Panpan Li, Wanying Ying, Hongxuan Li, Xiaohong Liu, Huidi Zhou, Jianmin Chen, Wengen Ouyang, Li Ji

AI总结:

通过无序/晶体异质界面实现稳定超润滑,利用DLC和MoS2界面非协调性及MXene增强,实现100000次摩擦循环中摩擦系数为0.008的高性能。

摘要:

摩擦消耗了全球大量能源,推动了超润滑(近零摩擦)在现实系统中的研究。传统方法依赖晶体晶格不匹配抑制周期性能量障碍,但真实界面不可避免地包含缺陷、边缘和晶界,恢复高摩擦状态。本文提出一种材料无关策略,基于无序/晶体异质界面实现工程相关条件下稳健的超润滑。使用类金刚石碳(DLC)和晶体MoS2作为模型系统,通过实验和原子模拟表明,其界面在所有取向下保持非协调,并在摩擦过程中表现出消失的能量障碍。相比之下,扭曲的MoS2双层容易重新定向为协调、高摩擦状态。通过制造激光雕刻的DLC/MoS2元接触阵列,并用Ti3C2Tx MXene增强,形成分层界面,在毫米级接触尺寸、12.7 GPa接触压力和40% RH空气的联合极端条件下,摩擦系数维持在~0.008。这种前所未有的性能源于四个协同因素:无序/晶体界面的内在非协调性、DLC支撑的刚性、基于MXene的机械增强以及通过几何图案化实现的负载分布标准化。这些发现建立了一种通用设计范式,将结构超润滑从纳米级模型系统扩展到可持续工程的实际技术。

英文摘要:

Friction dissipates a substantial portion of global energy, motivating the pursuit of superlubricity, a state of near-zero friction, in real-world systems. Conventional approaches rely on crystalline lattice mismatch to suppress periodic energy barriers, but real interfaces invariably contain defects, edges and grain boundaries that restore high-friction states. Here we introduce a materials-agnostic strategy based on amorphous/crystalline heterointerfaces to achieve robust superlubricity under engineering-relevant conditions. Using diamond-like carbon (DLC) and crystalline MoS2 as a model system, we show through experiments and atomistic simulations that their interface remains incommensurate at all orientations and exhibits vanishing energy barriers during friction. In contrast, twisted MoS2 bilayers readily reorient into commensurate, high-friction states. We scale this effect by fabricating laser-patterned arrays of DLC/MoS2 meta-contacts reinforced with Ti3C2Tx MXene, forming hierarchical interfaces that sustain a friction coefficient of ~0.008 over 100000 cycles under combined extreme conditions: millimetre-scale contact size, 12.7 GPa contact pressure and RH 40% air. This unprecedented performance arises from four synergistic factors: intrinsic incommensurability at amorphous/crystalline interface, the rigidity of DLC support, MXene-based mechanical reinforcement and normalized load distribution by geometric patterning. These findings establish a general design paradigm that extends structural superlubricity from nanoscale model systems to practical technologies for sustainable engineering.