arXiv 2603.11913cond-mat.mtrl-sci
收藏

超快激光激发后铁薄片中深度分辨的磁化动力学

Depth-resolved magnetization dynamics in Fe thin films after ultrafast laser excitation

Sorbonne Université(索邦大学);CNRS(法国国家科学研究中心);Synchrotron SOLEIL(SOLEIL同步辐射中心);Deutsches Elektronen-Synchrotron(德国电子同步辐射研究所);Laboratoire Albert Fert(阿尔伯特·费尔特实验室);Thales(泰雷兹集团);Université Paris-Saclay(巴黎萨克雷大学);Max Born Institut für Nichtlineare Optik und Kurzzeitspektroskopie(马克斯·玻恩非线性光学和超快光谱学研究所)
Valentin Chardonnet, Marcel Hennes, Romain Jarrier, Renaud Delaunay, Nicolas Jaouen, Marion Kuhlmann, Cyril Leveillé, Clemens von Korff Schmising, Daniel Schick… 展开作者

Valentin Chardonnet, Marcel Hennes, Romain Jarrier, Renaud Delaunay, Nicolas Jaouen, Marion Kuhlmann, Cyril Leveillé, Clemens von Korff Schmising, Daniel Schick, Kelvin Yao, Xuan Liu, Gheorghe S. Chiuzbăian, Jan Lüning, Boris Vodungbo, Emmanuelle Jal

AI总结:

研究超快激光激发后铁薄片中磁化动力学,揭示局部和非局部角动量转移现象及磁化弛豫与厚度振荡机制。

摘要:

我们对激光激发的铁磁性铁薄片进行了时间分辨X射线共振磁反射测量,以同时探测瞬时的结构和磁性深度分布,空间分辨率为纳米,时间分辨率为飞秒。我们的结果表明,在光学激发后的前皮秒内,铁层的磁化强烈不均匀,特别是在埋藏界面附近。通过将实验结果与基于微观三温模型的预测以及激光诱导自旋电流的模拟进行比较,我们证明了局部和非局部角动量转移现象同时发生。几皮秒后,磁化逐渐恢复到平衡状态,而整个薄片厚度开始周期性振荡,由于激光诱导应力,最大膨胀约为整个薄片厚度的1.3%。

英文摘要:

We performed time-resolved x-ray resonant magnetic reflectivity measurements on a laser-excited ferromagnetic Fe thin film to simultaneously probe the transient magnetic and structural depth profiles with nanometer spatial and femtosecond temporal resolution. Our results show that during the first picoseconds after optical excitation, the magnetization of the Fe layer is strongly inhomogeneous, especially in the vicinity of the buried interface. By comparing our experimental results to predictions based on the microscopic three-temperature model and simulations of laser-induced spin-currents, we demonstrate that local and non-local angular momentum transfer phenomena take place simultaneously. After a few picoseconds, the magnetization relaxes back to equilibrium while the total thin film thickness starts oscillating periodically, with a maximum dilation of approximately 1.3% of the entire thin film thickness due to laser-induced stresses.