优化兼容CMOS的超导氧化钛谐振器:沉积条件和结构化工艺
Optimizing CMOS-compatible, superconducting titanium nitride resonators: Deposition conditions and structuring processes
AI总结:
通过优化沉积和蚀刻工艺,实现了低至$9.67 \times 10^{-7}$的TLS损耗,为CMOS兼容的超导TiN谐振器提供了低损耗制造方案。
摘要:
我们报告了基于在200毫米直径高电阻率Si(100)基底上沉积的氧化钛(TiN)薄膜的超导同平面波导(CPW)谐振器的制造和表征。我们系统地研究了沉积条件、干蚀刻功率和原位电阻剥离温度如何影响形态、超导性质和介电损耗。通过调节反应溅射条件,实现了三种不同的首选晶向——(111)、(200)和混合。我们的结果表明,所有表现出相似最低的双能级系统(TLS)损耗的薄膜中,TiN111表现出最低的中位TLS损耗$\tildeδ_\mathrm{TLS}$,并且对再氧化具有更大的鲁棒性。相比之下,应用的结构化工艺对TLS损耗的影响远大于TiN薄膜的晶向和由此导致的超导层内在材料性质。所有TiN沉积物中最低的TLS损耗是通过低功率蚀刻和低温度电阻剥离实现的。此外,缓冲氧化蚀刻(BOE)处理可以去除金属-空气(MA)和基底-空气(SA)界面的高损耗氧化层,并恢复蚀刻引起的TLS损耗。因此,实现了TLS损耗值为$9.67 \times 10^{-7}$的TiN谐振器。相应的中位低功率损耗$\tildeδ_\mathrm{LP}$为$11.04 \times 10^{-7}$,相当于内部品质因子接近一百万。这些发现突显了过程诱导的氧化层在MA和SA界面限制TiN谐振器性能的关键作用,并提供了一种可扩展、低损耗的工艺,与工业级200毫米CMOS量子比特制造流程兼容。
英文摘要:
We report on the fabrication and characterization of superconducting coplanar waveguide (CPW) resonators based on titanium nitride (TiN) thin films deposited on 200\,mm diameter high-resistivity Si(100) substrates. We systematically investigate how deposition conditions, dry-etch power and in-situ resist strip temperature affect morphology, superconducting properties and dielectric losses. By tuning reactive sputtering conditions, three distinct preferred out-of-plane crystal orientations - (111), (200), and a mix of both are achieved. Our results demonstrate that all films exhibit similar minimal two-level system (TLS) losses, with TiN111 exhibiting the lowest median TLS losses $\tildeδ_\mathrm{TLS}$, and greater robustness against reoxidation. The applied structuring process, in contrast, has a far greater influence on the TLS loss than the crystal orientation of the TiN film and, consequently, the intrinsic material properties of the superconducting layer. The lowest TLS losses for all TiN depositions were achieved with a low power etch and low temperature resist strip. An additional buffered oxide etch (BOE) treatment could remove high-loss interfacial oxides at the metal-air (MA) and substrate-air (SA) interface and recover the etch-induced TLS losses. Consequently, TiN resonators exhibiting $\tildeδ_\mathrm{TLS}$ values as low as $9.67 \times 10^{-7}$ were realized. The corresponding median low-power loss, $\tildeδ_\mathrm{LP}$, amounts to $11.04 \times 10^{-7}$, which translates to an internal quality factor approaching one million. These findings highlight the critical role of process induced oxide formation at the MA and SA interfaces in limiting the performance of TiN resonators and provide a scalable, low-loss process compatible with industry-grade 200\,mm CMOS qubit fabrication workflows.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。