研究发现通过退火温度调节可显著提升Hf-Nb-Sc-Ti-Zr共晶高熵合金的超导临界温度,并发现其强耦合超导特性。

摘要:

当前对共晶高熵合金(HEA)Hf-Nb-Sc-Ti-Zr系统的超导性质的研究揭示了在体心立方(bcc)相中超导临界温度(T_c)相比典型的五元bcc高熵合金有所增强。在Hf₁₀Nb₂₅Sc₂₅Ti₂₀Zr₂₀、Hf₅Nb₄₅Sc₂₀Ti₁₅Zr₁₅和Hf₅Nb₄₅Sc₁₀Ti₅Zr₃₅系统中,这些系统涵盖了广泛的每个原子的价电子浓度、晶格应变以及部分或不存在共晶相的特征,在较低的退火温度下。在所有系统中,退火温度达到600°C后,共晶区域迅速扩展。每个系统的T_c随着退火温度从400°C上升到600°C显著增加,达到最大值9.93 K,在800°C退火的Hf₅Nb₄₅Sc₁₀Ti₅Zr₃₅样品中。几乎所有样品都可以归类为强耦合超导体。在Hf₅Nb₄₅Sc₁₀Ti₅Zr₃₅系统中退火温度为500°C的样品,在4.2 K时,临界电流密度(J_c)超过10⁵ A/cm²的实用阈值,达到约4 T,2 K时达到6 T。升高的J_c归因于显著的晶格应变和相不稳定性。通过比热数据的分析,研究了Hf-Nb-Sc-Ti-Zr系统中T_c增强的潜在机制,表明热退火引起的共晶区域的扩展起着关键作用。

英文摘要:

The present investigation into the superconducting properties of eutectic high-entropy alloy (HEA) Hf-Nb-Sc-Ti-Zr systems reveals an enhanced superconducting critical temperature ($T_\mathrm{c}$) in body-centered cubic (bcc) phases compared to typical quinary bcc HEAs. In Hf$_{10}$Nb$_{25}$Sc$_{25}$Ti$_{20}$Zr$_{20}$, Hf$_{5}$Nb$_{45}$Sc$_{20}$Ti$_{15}$Zr$_{15}$, and Hf$_{5}$Nb$_{45}$Sc$_{10}$Ti$_{5}$Zr$_{35}$ systems, which span a broad range of valence electron concentration per atom, lattice strain and the presence of partial or absent eutectic phases are characteristic features at lower annealing temperatures. The eutectic regions expand rapidly following annealing at 600$^{\circ}$C in all systems. The $T_\mathrm{c}$ of each system increases markedly with rising annealing temperatures from 400$^{\circ}$C to 600$^{\circ}$C, reaching a maximum value of 9.93 K in the Hf$_{5}$Nb$_{45}$Sc$_{10}$Ti$_{5}$Zr$_{35}$ sample annealed at 800$^{\circ}$C. Nearly all samples can be classified as strong-coupling superconductors. The sample annealed at 500$^{\circ}$C in the Hf$_{5}$Nb$_{45}$Sc$_{10}$Ti$_{5}$Zr$_{35}$ system exhibits a critical current density ($J_\mathrm{c}$) exceeding the practical threshold of 10$^{5}$ A/cm$^{2}$ up to approximately 4 T at 4.2 K and 6 T at 2 K. The elevated $J_\mathrm{c}$ is attributed to significant lattice strain and phase instability. The underlying mechanism for the enhanced $T_\mathrm{c}$ in Hf-Nb-Sc-Ti-Zr systems is examined through specific heat data analysis, suggesting that the expansion of the eutectic regions induced by thermal annealing plays a pivotal role.