arXivDaily arXiv每日学术速递 周一至周五更新
感恩节,周五至周末无更新,大家顺遂。周一再来吧
arXiv 2502.02203cond-mat.mtrl-sci
收藏

La$_{2-x}A'_{x}$Ni$_{7}$化合物($A'$ = Sm, Gd)的多晶型结构与磁性能之间的关系

Relationship between polymorphic structures and magnetic properties of La$_{2-x}A'_{x}$Ni$_{7}$ compounds ($A$' = Sm, Gd)

Valérie Paul-Boncour, Véronique Charbonnier, Nicolas Madern, Lotfi Bessais, Judith Monnier, Junxian Zhang

AI总结:

本研究通过X射线衍射和磁性测量,揭示了La$_{2-x}A'_{x}$Ni$_{7}$($A'$=Sm, Gd)的多晶型结构(2H/3R)与磁性能的关联,发现Sm掺杂产生硬磁行为,Gd掺杂产生软铁磁行为。

摘要:

本研究结合X射线粉末衍射和磁性测量,研究了含磁性稀土元素($A'$ = Sm, Gd)的La$_{2-x} A'_{x}$Ni$_{7}$化合物的晶体结构和磁性能。这些共生化合物结晶为2$H$六方(Ce$_{2}$Ni$_{7}$型)和3$R$菱方(Gd$_{2}$Co$_{7}$型)多晶型结构的混合物,这两种结构都与[$AB_{5}$]和[$A_{2}B_{4}$]亚单元沿$c$轴的堆叠有关。平均晶胞体积随$A'$含量线性减小,而$c/a$比值在$x$ = 1时达到最小值,这是由于$A'$替代La时两个不同亚单元之间的几何约束所致。磁性能强烈依赖于结构类型和$A'$含量。六方La$_{2}$Ni$_{7}$在低场和低温下是弱反铁磁体(wAFM),并在施加场下经历变磁转变至弱铁磁态(wFM)。在0.1 T的施加场下,La$_{2-x}A'_{x}$Ni$_{7}$金属间化合物显示出两个不同的转变温度$T_{1}$和$T_{2}$,两者均随$x$增加而升高。$T_{1}$与2$H$相中$A'$= Sm时的wFM-wAFM转变相关,而$T_{2}$与2$H$和3$R$相的居里温度相关。在$T_{1}$和$T_{2}$之间观察到变磁行为,对于$A'$ = Sm的化合物,转变场$μ_{0}H_{Trans}$在2至3.5 T之间。La$_{2-x}Sm_{x}$Ni$_{7}$化合物($x$ > 0)表现为硬磁体,在低温下具有大的矫顽场$μ_{0}H_{C}$(对于$x$ = 2,在5 K时$μ_{0}H_{C}$ > 9 T),而La$_{2-x} Gd_{x}$Ni$_{7}$化合物($x$ > 0)是软铁磁体,饱和磁化强度随Gd含量线性增加。

英文摘要:

In this study, the crystal structure and magnetic properties of La$_{2-x} A'_{x}$Ni$_{7}$ compounds with magnetic rare earth elements ($A$' = Sm, Gd) have been investigated combining X-ray powder diffraction and magnetic measurements. These intergrowth compounds crystallize in a mixture of 2$H$ hexagonal (Ce$_{2}$Ni$_{7}$-type) and 3$R$ rhombohedral (Gd$_{2}$Co$_{7}$-type) polymorphic structures which are related to the stacking of [$AB_{5}$] and [$A_{2}B_{4}$] subunits along the $c$-axis.The average cell volume decreases linearly versus $A$' content, whereas the $c/a$ ratio reaches a minimum at $x$ = 1, due to geometric constraints upon $A$' for La substitution between the two different subunits. The magnetic properties strongly depend on the structure type and the $A$' content. Hexagonal La$_{2}$Ni$_{7}$ is a weak antiferromagnet (wAFM) at low field and temperature and undergoes metamagnetic transitions towards weak ferromagnetic state (wFM) under applied field. Under an applied field of 0.1 T, La$_{2-x}A'_{x}$Ni$_{7}$ intermetallic compounds display two different transition temperatures $T_{1}$ and $T_{2}$ that both increase with $x$. $T_{1}$ is associated with a wFM-wAFM transition in the 2$H$ phase for $A$'= Sm, whereas $T_{2}$ is related to the Curie temperature of both 2$H$ and 3$R$ phases. A metamagnetic behaviour is observed between $T_{1}$ and $T_{2}$ with transition field $μ_{0}H_{Trans}$ between 2 and 3.5 T for compounds with $A$' = Sm. The La$_{2-x}Sm_{x}$Ni$_{7}$ compounds ($x$ > 0} behave as hard magnets with a large coercive field $μ_{0}H_{C}$ at low temperature ($μ_{0}H_{C}$ > 9 T at 5 K for $x$ = 2), whereas the La$_{2-x} Gd_{x}$Ni$_{7}$ compounds ($x$ > 0) are soft ferrimagnets with a linear increase of the saturation magnetization versus Gd content.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑