Mischemal成分和冷却速率对Al-(Ce, La, Nd)共晶合金显微结构和力学性能的影响
Effects of Mischmetal Composition and Cooling Rates on the Microstructure and Mechanical Properties of Al-(Ce, La, Nd) Eutectic Alloys
AI总结:
研究通过替换Ce为MM,探讨了Al-MM合金显微结构和力学性能的影响,发现Al-9MM具有优异的粗化抗性和环境效益,表现出良好的应用前景。
摘要:
本研究探讨了在铸造Al-MM合金中用Mischemal(MM)替代铈(Ce)的影响,重点研究了显微结构、硬度、拉伸和压缩性能、蠕变抗力和粗化抗力。具有不同MM成分(Ce、Ce-50La、Ce-33La和Ce-27La-19Nd,重量百分比)的Al-MM合金表现出近共晶和超共晶显微结构,分别对应于Al-9MM和Al-12MM成分,其铸态硬度相似(约525 MPa)。所有Al-9MM合金的拉伸屈服应力约为55 MPa,抗拉强度约为130 MPa,断裂伸长率约为8%。显微结构和力学性能的一致性表明MM成分在Al-MM合金中的灵活性。Al-9MM表现出优异的粗化抗性,当暴露在300和350°C下长达11周时,硬度减少最小,而在400°C下暴露8周时硬度仅减少约15%,优于共晶Al-12.6Si和Al-6.4Ni合金。此外,Al-9MM在300°C下的蠕变抗性优于大多数沉淀强化的Al-Sc-Zr和固溶强化的Al-Mg/Mn合金,但不如共晶强化的Al-6.4Ni和Al-10Ce-5Ni合金。通过楔形铸造研究了铸造冷却速率的影响:Al-9Ce在冷却速率降低时从亚共晶转变为超共晶,而Al-12Ce始终表现出超共晶显微结构。Al11Ce3层状结构随着冷却速率的增加而变细且更紧密排列。Al-9Ce在高到中等冷却速率下保持稳定的硬度,但在较低冷却速率下硬度降低,而Al-12Ce的硬度没有变化。在减少15%的能耗和CO2排放的情况下,用MM替代Ce的Al-Ce合金具有可比的机械性能和增强的环境效益,突显了MM作为可持续替代品的潜力。
英文摘要:
This study investigates the substitution of cerium (Ce) with mischmetal (MM) in cast Al-MM alloys, focusing on microstructure, hardness, tensile and compression properties, creep resistance, and coarsening resistance. Al-MM alloys with various MM compositions (Ce, Ce-50La, Ce-33La, and Ce-27La-19Nd, weight percent) exhibit near-eutectic and hyper-eutectic microstructures for Al-9MM and Al-12MM compositions, respectively, with similar as-cast hardness (~525 MPa). All Al-9MM alloys show tensile yield stress ~55 MPa, ultimate tensile strength ~130 MPa, and fracture strain ~8%.The microstructural and mechanical properties consistency demonstrates the flexibility of MM compositions in Al-MM alloys. Al-9MM exhibits excellent coarsening resistance, with minimal hardness reduction when exposed to 300 and 350 C for up to 11 weeks, and a modest ~15% hardness reduction at 400 C for 8 weeks, outperforming eutectic Al-12.6Si and Al-6.4Ni alloys. Additionally, Al-9MM shows higher creep resistance at 300 C compared to most precipitate-strengthened Al-Sc-Zr and solid-solution-strengthened Al-Mg/Mn alloys, but is outperformed by eutectic-strengthened Al-6.4Ni and Al-10Ce-5Ni alloys.The effect of casting cooling rate is investigated through wedge casting: Al-9Ce transitions from hypo- to hyper-eutectic as cooling rates decrease, while Al-12Ce consistently shows hyper-eutectic microstructures. Al11Ce3 lamellae become finer and more closely spaced with increasing cooling rates. Al-9Ce maintains steady hardness at high to moderate cooling rates but shows reduced hardness at lower rates, whereas Al-12Ce shows no change in hardness.With a 15% reduction in energy consumption and CO2 emissions, Al-Ce alloys where Ce is replaced with MM offer comparable mechanical properties and enhanced environmental benefits, highlighting the potential of MM as a sustainable alternative.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。