arXivDaily arXiv每日学术速递 周一至周五更新
arXiv 2408.02863cond-mat.mtrl-sciquant-ph
收藏

通过氟化铵蚀刻提升超导量子比特性能

Enhanced Superconducting Qubit Performance Through Ammonium Fluoride Etch

Cameron J. Kopas, Dominic P. Goronzy, Thang Pham, Carlos G. Torres Castanedo, Matthew Cheng, Rory Cochrane, Patrick Nast, Ella Lachman, Nikolay Z. Zhelev, Andre… 展开作者

Cameron J. Kopas, Dominic P. Goronzy, Thang Pham, Carlos G. Torres Castanedo, Matthew Cheng, Rory Cochrane, Patrick Nast, Ella Lachman, Nikolay Z. Zhelev, Andre Vallieres, Akshay A. Murthy, Jin-su Oh, Lin Zhou, Matthew J. Kramer, Hilal Cansizoglu, Michael J. Bedzyk, Vinayak P. Dravid, Alexander Romanenko, Anna Grassellino, Josh Y. Mutus, Mark C. Hersam, Kameshwar Yadavalli

AI总结:

本文提出用氢氟酸加氟化铵水溶液的湿化学蚀刻替代BOE清洗,处理约瑟夫森结-衬底及衬底-空气界面,使超导量子比特中位T1提高约22%,TLS损耗角正切降低约33%,并通过界面表征揭示了可能的微观机制。

摘要:

超导量子比特的性能通常受到耗散和双能级系统(TLS)损耗的限制。这些损耗的主要来源被认为来自非晶材料以及界面和表面处的缺陷,很可能是制造工艺或环境暴露的结果。在此,我们探索了一种新颖的湿化学表面处理方法,作用于约瑟夫森结-衬底界面和衬底-空气界面,用氢氟酸后接氟化铵水溶液的工艺替代缓冲氧化物蚀刻(BOE)清洗工艺。我们表明,氟化铵蚀刻工艺使中位$\ ext{T}_1$在统计上显著提高了约22%($p=0.002$),并减少了可调频率范围内强耦合TLS的数量。对在铌沉积前经过氟化铵蚀刻处理的样品进行的微波谐振器测量也显示,与BOE处理的样品相比,TLS引起的损耗角正切降低了约33%。由于该化学处理主要改变约瑟夫森结-衬底界面和衬底-空气界面,我们进行了针对性的化学和结构表征,以考察这些界面处的材料差异,并识别出多种可能导致TLS减少的微观变化。

英文摘要:

The performance of superconducting qubits is often limited by dissipation and two-level systems (TLS) losses. The dominant sources of these losses are believed to originate from amorphous materials and defects at interfaces and surfaces, likely as a result of fabrication processes or ambient exposure. Here, we explore a novel wet chemical surface treatment at the Josephson junction-substrate and the substrate-air interfaces by replacing a buffered oxide etch (BOE) cleaning process with one that uses hydrofluoric acid followed by aqueous ammonium fluoride. We show that the ammonium fluoride etch process results in a statistically significant improvement in median $\text{T}_1$ by $\sim22\%$ ($p=0.002$), and a reduction in the number of strongly-coupled TLS in the tunable frequency range. Microwave resonator measurements on samples treated with the ammonium fluoride etch prior to niobium deposition also show $\sim33\%$ lower TLS-induced loss tangent compared to the BOE treated samples. As the chemical treatment primarily modifies the Josephson junction-substrate interface and substrate-air interface, we perform targeted chemical and structural characterizations to examine materials' differences at these interfaces and identify multiple microscopic changes that could contribute to decreased TLS.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑