研究了真空退火对钇铁石榴石(YIG)Gilbert阻尼的影响,发现300 C真空退火使阻尼增加8倍,而氧气环境下无变化,该效应在自旋泵浦测量中需被考虑。

摘要:

研究了在覆盖金属层之前,热表面清洁对钇铁石榴石(YIG)的Gilbert阻尼$α$的影响。结果表明,在真空中进行相对温和的退火条件(T = 300 C)时,$α$受到强烈影响。在通过自旋泵浦测量获取自旋混合电导率时,需要考虑这种增加。当YIG在300 C下真空退火时,我们测得$α$增加了8倍。在0.1 mbar的氧气中于相同温度下退火时,未观察到$α$的此类变化。

英文摘要:

The effect of thermal surface cleaning on the Gilbert damping, $α$, of yttrium iron garnet (YIG), before capping with a metallic layer, has been investigated. Our results show that $α$ is strongly effected by relatively mild annealing conditions (T = 300 C) when performed in a vacuum. This increase needs to be taken into account when obtaining the spin mixing conductance from spin pumping measurements. We measure an increase in $α$ by a factor of 8 when the YIG is vacuum annealed at 300 C. No such changes in $α$ are observed when annealed at the same temperature in 0.1 mbar of oxygen.

机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。

↑