化学成分对C15 Ca-Al-Mg Laves相室温塑性的影响
Influence of chemical composition on the room temperature plas-ticity of C15 Ca-Al-Mg Laves phases
AI总结:
通过纳米压痕和原子模拟研究了Mg和Ca添加对C15 CaAl2 Laves相室温力学性能的影响,发现成分变化会改变硬度、模量及多种{11n}滑移系的激活机制。
摘要:
研究了化学成分变化对C15 CaAl2 Laves相室温力学性能的影响,考察了两种非化学计量比成分:添加5.7 at.-% Mg的Ca33Al61Mg6,以及添加10.8 at.-% Mg和3.0 at.-% Ca的Ca36Al53Mg11,并与化学计量比成分Ca33Al67进行对比。采用纳米压痕对具有多种结晶学取向的立方Ca-Al-Mg Laves相进行了表征和变形测试。测得Ca36Al53Mg11的硬度和压痕模量分别为4.1 ± 0.3 GPa和71.3 ± 1.5 GPa,Ca33Al61Mg6分别为4.6 ± 0.2 GPa和80.4 ± 3.8 GPa,Ca33Al67分别为4.9 ± 0.3 GPa和85.5 ± 4.0 GPa。在压痕表面上区分了产生的表面痕迹以及滑移面和裂纹面,揭示了多种不同{11n}滑移系的激活,常规透射电子显微镜观察进一步证实了这一点。此外,通过原子模拟评估了激活滑移系的变形机制及相应的能垒。
英文摘要:
The influence of chemical composition changes on the room temperature mechanical proper-ties in the C15 CaAl2 Laves phase were investigated in two off-stoichiometric compositions with 5.7 at.-% Mg addition (Ca33Al61Mg6) and 10.8 at.-% Mg and 3.0 at.-% Ca addition (Ca36Al53Mg11) and compared to the stoichiometric (Ca33Al67) composition. Cubic Ca-Al-Mg Laves phases with multiple crystallographic orientations were characterised and deformed using nanoindentation. The hardness and indentation modulus were measured to be 4.1 +- 0.3 GPa and 71.3 +- 1.5 GPa for Ca36Al53Mg11, 4.6 +- 0.2 GPa and 80.4 +- 3.8 GPa for Ca33Al61Mg6 and 4.9 +- 0.3 GPa and 85.5 +- 4.0 GPa for Ca33Al67, respectively. The resulting surface traces as well as slip and crack planes, were distinguished on the indentation surfac-es, revealing the activation of several different {11n} slip systems, as further confirmed by conventional transmission electron microscopic observations. Additionally, the deformation mechanisms and corresponding energy barriers of activated slip systems were evaluated by atomistic simulations.
机构、总结、中文摘要均由AI分析而来,可能存在错误,请以论文正文为准。